Material Notes:
Semiconductive/dissipative product based on Polyoxymethylene (POM). Carbon nanotubes.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.419 g/cc
0.05126 lb/in³
Linear Mold Shrinkage, Flow 0.020 - 0.0235 cm/cm
0.020 - 0.0235 in/in
Linear Mold Shrinkage, Transverse 0.0205 - 0.0225 cm/cm
0.0205 - 0.0225 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
Elongation at Break 10 %
10 %
Tensile Modulus 2.90 GPa
421 ksi
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Vicat Softening Point 150 °C

@Load 5.00 kg
302 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 ohm-cm
1.00e+8 ohm-cm
Surface Resistance 3.00e+7 ohm
3.00e+7 ohm
Processing Properties Metric English Comments
Melt Temperature 180 - 200 °C
356 - 392 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 - 100 °C

@Time 10800 sec
176 - 212 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa