Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SIDPEC EGYPTENE® HD 5813 EA HDPE Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer SIDPEC (Sidi Kerir Petrochemicals Co.)
Trade Name EGYPTENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SIDPEC EGYPTENE® HD 5813 EA HDPE Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications:CrateAerosol capsHouse waresInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ISO 1872/1
Environmental Stress Crack Resistance 50 hour

@Temperature 23.0 °C
50 hour

@Temperature 73.4 °F
F<sub>50</sub>; ASTM D1693
Melt Flow 13 g/10 min

@Load 2.16 kg
13 g/10 min

@Load 4.76 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
BP 13B/1
Elongation at Break >= 1000 %
>= 1000 %
BP 13B/1
Flexural Modulus 1.10 GPa
160 ksi
ISO 178-1975
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179