Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Atom Adhesives AA-CARB 61 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-CARB 61 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AA-CARB 61 is an epoxy adhesive and coating formulation based on conductive carbon. AA-CARB 61 is recommended for electronic bonding and sealing applications that require both fine electrical and mechanical properties. AA-CARB 61 cures at room temperature or can be accelerated with mild heat to form a tenacious bond between similar and dissimilar substrates.Appearance: BlackCure Type: Heat cure or Room temperature Benefits:Continuity of conductivityHigh adhesionWide operating temperature range Substrates: Aluminum, copper, magnesium, steel, bronze, nickel, ceramic, glass, phenolic, G-10 epoxy glass boards Typical Application: Electronic bonding and sealing applications that require both fine electrical and mechanical properties.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
mixed, uncured
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Tensile Strength 65.5 MPa
9500 psi
Compressive Strength 89.6 MPa
13000 psi
uncured
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C
8.33 µin/in-°F
Thermal Conductivity 1.22 W/m-K
8.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 170 °C
338 °F
Heat Distortion Temperature 95.0 °C
203 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 40 ohm-cm
<= 40 ohm-cm
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 100 °C
0.250 hour

@Temperature 212 °F
60.0 min

@Temperature 60.0 °C
1.00 hour

@Temperature 140 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30.0 min
30.0 min
100g, uncured
Shelf Life 12.0 Month
12.0 Month
uncured
Descriptive Properties Value Comments
Viscosity Paste
uncured
Users viewing this material also viewed the following: