3M Dyneon™ ET 6235Z Fluorothermoplastic Granules

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE
Manufacturer 3M Dyneon™
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ ET 6235Z Fluorothermoplastic Granules.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ET 6235 is a melt-processable fluoroplastic consisting mainly of alternating tetrafluoroethylene and ethylene monomer units (ETFE). Applications: Its excellent properties make Dyneon ET 6235Z ideal for use in a wide variety of industries, including applications in the electronics, chemical processing, laboratory testing equipment and outdoor architectural structure industries. It can be easily fabricated into films, extruded thin-walled tubing and injection molded parts.This partially crystalline fluorothermoplastic offers a valuable combination of properties:Wide service temperature range -200° to +150°CLow flammabilityExcellent electrical and mechanical propertiesVery good resistance to solvents and chemicalsExtremely high resistance to outdoor weatheringHigh light transmission in the visible and UV rangesNon-stick characteristicsExcellent tear resistanceLow permeabilityGood resistance to radiationInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.73 g/cc
1.73 g/cc
ASTM D792
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 297 °C
10 g/10 min

@Load 11.0 lb,
Temperature 567 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 MPa
6670 psi
ASTM D638
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 425 %
425 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 267 °C
513 °F
ASTM D4591
Maximum Service Temperature, Air 150 °C
302 °F
DIN 57207 part 6
Minimum Service Temperature, Air -200 °C
-328 °F
Flammability, UL94 V-0
V-0
Oxygen Index >= 30 %
>= 30 %
ASTM D2863
Optical Properties Metric English Comments
Transmission, Visible >= 90 %

@Wavelength 380 - 780 nm,
Thickness 0.100 mm
>= 90 %

@Wavelength 380 - 780 nm,
Thickness 0.00394 in
film
Electrical Properties Metric English Comments
Dielectric Constant 2.58

@Frequency 1e+6 Hz
2.58

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 150 kV/mm
3810 kV/in
0.1 mm; ASTM D149
Descriptive Properties Value Comments
Flame Rating (110 µm film) Building Material Class B1