Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.640 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.640 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Maxxam™ PPC-20G Black Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Izod Impact, Notched 0.640 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ 600 A Natural Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
Izod Impact, Notched 0.640 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Therma-Tech™ NJ-6000 TC Polyamide 12 (Nylon 12)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass
ABS is highly resistant to weak acids and alkalis, and provides good resistance to most organic solvents. It is attacked by sulfuric and nitric acids, and is soluble in esters, ketones and ethylene ..
Izod Impact, Notched 0.640 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
PTS Trimid® N6-200L Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 0.640 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ ND 1233 GF Black Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert..
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Albis Plastics Polypropylene A 12 H-GK20/GF20 C , 20% Glass Bead/20% Glass Fiber  (discontinued **)
Semi-crystalline Polypropylene Homopolymer (PPHP)Characteristics: Chemically Coupled Fiber; Good Dimensional StabilityApplications: Appliances, Furniture, Cases, Packaging and NoveltiesProcessing: I..
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics ULTEM 4000 PEI
Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing.
Izod Impact, Notched 0.640 J/cm

@Temperature -30.0 °C
1.20 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics ULTEM HU2110 PEI
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP ..
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON DSL229 PC (Asia Pacific)
LNP* Stat-kon* DSL229 is a compound based on Polycarbonate resin containing PTFE, Stainless Steel. Added features of this material include: Electrically Conductive, Internally Lubricated.
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Valox® EF4530 PBT (Asia Pacific)
Easy flow, 30% glass-reinforced, PBTP resin. Flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP PF005S PA 6 (Asia Pacific)
LNP* Thermocomp* PF005S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RF0069SF PA 66 (Asia Pacific)
LNP* Thermocomp* RF0069SF is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP UF0067W PPA
LNP* THERMOCOMP* UF0067W is a compound based on Polyphthalamide resin containing 30% glass fiber. Added features of this material include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flam..
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific)
LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RFZ349XC PA 66 (Asia Pacific)
LNP* THERMOCOMP* RFZ349XC is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant.
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black
DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman.
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black
DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman.
Izod Impact, Notched 0.640 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Entec Hypro™ PPC-CC40 Natural Copolymer Polypropylene, 40% Calcium Carbonate Filled
Information provided by Entec
Izod Impact, Notched 0.640 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Entec Hypro™ PPH-GF10 Natural Homopolymer Polypropylene, 10% Glass Reinforced
Information provided by Entec
Izod Impact, Notched 0.640 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers NPP20-1201CAS Random Copolymer Polypropylene (Clarified, with Antistat)
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 62M Nylon 66, 40% Mineral reinforced
A 40% mineral reinforced Nylon 66 resin modified for reduced shrinkage.Data provided by the manufacturer
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 982 Nylon 612
General purpose for extrusion. These resins are notes for their low moisture absorption and excellent dimensional stability. Bristle grade, high viscosity.Data provided by the manufacturer
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Chem Polymer Chemlon 113 G Nylon 66, 13% Glass Fiber Reinforced
A 13% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials.Data provided by the manufacturer, ..
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 538 Nylon 66
A general purpose high viscosity extrusion grade Nylon 66.Data provided by the manufacturer
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
A. Schulman ComAlloy Voloy® 113 Polypropylene, Glass Reinforced, Chemically Coupled, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.25% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp DFZ42P PC (Asia Pacific)
LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the..
Izod Impact, Notched 0.640 J/cm

@Thickness 6.35 mm
1.20 ft-lb/in

@Thickness 0.250 in
ASTM D256
PolyOne Stat-Tech™ RA-06CF-09GF/000 EM Polyarylsulfone - ESD Applications - Flow Enhanced Grade  (discontinued
Data provided by PolyOne.
Izod Impact, Notched 0.640 J/cm

@Diameter 3.17 mm
1.20 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
BP Amoco Acclear® 8649X Random Copolymer Polypropylene, High Clarity Grade  (discontinued **)
Developmental Grade. Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Low taste/odor, Excellent processabilityTypical applications: High clarity c..