| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Zytel® FE4200 BK136 Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.07 g/cc | 1.07 g/cc | DAM; ASTM D792 |
| Water Absorption | 0.98 % @Temperature 23.0 °C |
0.98 % @Temperature 73.4 °F |
Immersion 24h; DAM; ASTM D570 |
| Linear Mold Shrinkage | 0.015 cm/cm @Thickness 3.20 mm |
0.015 in/in @Thickness 0.126 in |
Transverse; DAM |
| 0.023 cm/cm @Thickness 3.20 mm |
0.023 in/in @Thickness 0.126 in |
Flow; DAM |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 70 | 70 | 50%RH; ASTM D785 |
| 106 | 106 | DAM; ASTM D785 | |
| Tensile Strength | 43.4 MPa @Temperature 23.0 °C |
6290 psi @Temperature 73.4 °F |
50%RH; ASTM D638 |
| 52.4 MPa @Temperature 23.0 °C |
7600 psi @Temperature 73.4 °F |
DAM; ASTM D638 | |
| Elongation at Break | 90 % @Temperature 23.0 °C |
90 % @Temperature 73.4 °F |
DAM; ASTM D638 |
| 200 % @Temperature 23.0 °C |
200 % @Temperature 73.4 °F |
50%RH; ASTM D638 | |
| Flexural Modulus | 0.331 GPa @Temperature 100 °C |
48.0 ksi @Temperature 212 °F |
DAM; ASTM D790 |
| 0.897 GPa @Temperature 23.0 °C |
130 ksi @Temperature 73.4 °F |
50%RH; ASTM D790 | |
| 1.862 GPa @Temperature 23.0 °C |
270.1 ksi @Temperature 73.4 °F |
DAM; ASTM D790 | |
| Izod Impact, Notched | 10.62 J/cm @Temperature 23.0 °C |
19.90 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
| Izod Impact, Unnotched | 10.6 J/cm @Temperature 23.0 °C |
19.9 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D4812 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 260 °C | 500 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| 260 °C | 500 °F | DAM; ASTM D3418 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | DAM; ISO 75-1/-2 |
| 98.0 °C | 208 °F | DAM; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 55.0 °C | 131 °F | DAM; ISO 75-1/-2 |
| 55.0 °C | 131 °F | DAM; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
| 280 - 300 °C | 536 - 572 °F | DAM | |
| Mold Temperature | 70.0 °C | 158 °F | DAM; optimum |
| 50.0 - 90.0 °C | 122 - 194 °F | DAM | |
| Drying Temperature | 80.0 °C | 176 °F | DAM |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
| Moisture Content | <= 0.20 % | <= 0.20 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Drying Recommended | Yes, if moisture content of resin exceeds recommended level | DAM |
| Forms | Pellets | DAM |
| Material Status | Preliminary Data | DAM |
| Processing Method | Extrusion | DAM |
| Product Category | Extrusion Resins | DAM |
| Toughened Resins | DAM | |
| Unreinforced Resins | DAM | |
| RoHS Compliance | Contact Manufacturer | DAM |