Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.07 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Noble Polymers Regis™ 285107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Specific Gravity 1.07 g/cc
1.07 g/cc
23/23°C; ASTM D792
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Polymer Resources NY66-IM2 Impact Modified Nylon 66
Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are ..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
PolyOne Stat-Tech™ AS-08CF/000 Black Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (disconti
Description/Features:Carbon Fiber ReinforcedESD ProtectionPolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
LG Chemical LI951 Heat Resistant ASA
Description: High Heat ASAApplication: Automotive Part (Radiator Grill, Side Mirror)CAS: 26299-47-8Information provided by LG Chemical
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
LG Chemical LUMID HI1202B(W) PA66, High Impact
Feature: Injection Molding, PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM 792
Multibase Multi-Flex® A 8103 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive Interior PartsInformation ..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
SABIC Innovative Plastics NORYL TN300 PPE+PS
PPE+PS. Transparent. High heat. Color Limited. Injection molding. Laser-Transmission welding applications.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
SABIC Innovative Plastics NORYL PX1712 PPE+HIPS (Asia Pacific)
PPE/HIPS unfilled high heat for auto interior
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Chase Plastics CP Pryme® ASA300 BK General Purpose (Utility) ASA Molding Resin
Information provided by Chase Plastics.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
A. Schulman POLYBATCH™ Orange 1096 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 1096 is an orange color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 1096 is he..
Specific Gravity 1.07 g/cc
1.07 g/cc
ISO 1183/1
A. Schulman POLYFORT™ FPP 1876 22% Mineral Filled Copolymer, UV Inhibited Polypropylene
DescriptionPolyfort® FPP 1876 is a 22% mineral filled copolymer UV Inhibited Polypropylene. It is high flow. Information provided by A. Schulman.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
A. Schulman POLYFLAM™ E-17338 22% CACO3 Filled Copolymer Polypropylene
DescriptionPolyfort® E 17338 is a 22% filled copolymer polypropylene product. Information provided by A. Schulman.
Specific Gravity 1.07 g/cc
1.07 g/cc
ISO 1183/1
A. Schulman POLYFORT™ FPP 1876 22% Mineral Filled Copolymer, UV Inhibited Polypropylene
DescriptionPolyfort® FPP 1876 is a 22% mineral filled copolymer UV Inhibited Polypropylene. It is high flow. Information provided by A. Schulman.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
A. Schulman POLYFLAM™ E-17338 22% CACO3 Filled Copolymer Polypropylene
DescriptionPolyfort® E 17338 is a 22% filled copolymer polypropylene product. Information provided by A. Schulman.
Specific Gravity 1.07 g/cc

@Temperature 25.0 °C
1.07 g/cc

@Temperature 77.0 °F
Dow Corning 804 RESIN
Maintenance paints, colored baking enamels, decorative finishes. As an additive to improve paint flow-out.Information provided by Dow Corning
Specific Gravity 1.07 g/cc

@Temperature 25.0 °C
1.07 g/cc

@Temperature 77.0 °F
Dow Corning HV 1520/40
40 Shore Hardness Conductive liquid silicone rubber with high tear strength, high electrical conductivity and fast cure speedInformation provided by Dow Corning
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
ELASTO UK Dryflex® 650700 TPE, Improved Compression Set and High Temperature Resistance, 70A Hardness
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Diamond Polymers ABS 4003HH
Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Diamond Polymers ABS 4107 Heat Resistant Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Diamond Polymers ASA S170
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Specific Gravity 1.07 g/cc
1.07 g/cc
Esstech X-943-7424 Triethyleneglycol Dimethacrylate, C14H22O6
Triethylene glycol dimethacrylate is a difunctional monomer that has been the foundation of many long-standing dental formulations. It has ideal water absorptivity and stability properties. Listed ..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Bhansali Engineering Santron IMS 2000 SAN Resin
Clear SANInformation provided by Bhansali
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Bhansali Engineering Santron IMS 2007LF SAN Resin
High Rigidity Clear SANInformation provided by Bhansali
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Bhansali Engineering Santron IMS1000M SAN Resin
Clear SAN, Pen barrel applicationInformation provided by Bhansali
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
A. Schulman POLYBLAK™ 2723Pm Premium Black Color Concentrate, 25% Carbon Black Based In HDPE
DescriptionPOLYBLAK® Black 2723 is a premium black color concentrate containing 25% carbon black in HDPE. This masterbatch is designed to maintain maximum impact strength and ESCR of the host HDPE..
Specific Gravity 1.07 g/cc
1.07 g/cc
Mixed; TM R050-16
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
Copyright © lookpolymers.com All Rights Reserved