| Category | Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/Nylon 6 Blend, Glass Fiber Filled |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® 70G35EF NC010 Nylon 66 + Nylon 6
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.24 g/cc | 0.0448 lb/in³ | |
| 1.40 g/cc | 0.0506 lb/in³ | DAM; ISO 1183 | |
| Water Absorption | 5.5 % @Thickness 2.00 mm |
5.5 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Moisture Absorption | 1.70 % @Thickness 2.00 mm |
1.70 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Viscosity | 43638 cP @Shear Rate 5000 1/s, Temperature 305 °C |
43638 cP @Shear Rate 5000 1/s, Temperature 581 °F |
ISO 11403-1 -2 |
| 52680 cP @Shear Rate 5000 1/s, Temperature 295 °C |
52680 cP @Shear Rate 5000 1/s, Temperature 563 °F |
ISO 11403-1 -2 | |
| 64549 cP @Shear Rate 5000 1/s, Temperature 285 °C |
64549 cP @Shear Rate 5000 1/s, Temperature 545 °F |
ISO 11403-1 -2 | |
| 124520 cP @Shear Rate 500 1/s, Temperature 305 °C |
124520 cP @Shear Rate 500 1/s, Temperature 581 °F |
ISO 11403-1 -2 | |
| 156800 cP @Shear Rate 500 1/s, Temperature 295 °C |
156800 cP @Shear Rate 500 1/s, Temperature 563 °F |
ISO 11403-1 -2 | |
| 198700 cP @Shear Rate 500 1/s, Temperature 285 °C |
198700 cP @Shear Rate 500 1/s, Temperature 545 °F |
ISO 11403-1 -2 | |
| Viscosity Test | 145 cm³/g | 145 cm³/g | DAM; ISO 307 1157 1628 |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 140 MPa | 20300 psi | 50%RH; ISO 527-1/-2 |
| 200 MPa | 29000 psi | DAM; ISO 527-1/-2 | |
| Tensile Stress | 7.61 MPa @Strain 0.150 %, Temperature 90.0 °C |
1100 psi @Strain 0.150 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
| 10.92 MPa @Strain 0.250 %, Temperature 150 °C |
1584 psi @Strain 0.250 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 11.43 MPa @Strain 0.280 %, Temperature 150 °C |
1658 psi @Strain 0.280 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 | |
| 15.04 MPa @Strain 0.270 %, Temperature 90.0 °C |
2181 psi @Strain 0.270 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 | |
| 19.29 MPa @Strain 0.300 %, Temperature 23.0 °C |
2798 psi @Strain 0.300 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 | |
| 20.06 MPa @Strain 0.330 %, Temperature 40.0 °C |
2909 psi @Strain 0.330 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 39.28 MPa @Strain 1.31 %, Temperature 150 °C |
5697 psi @Strain 1.31 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 | |
| 47.25 MPa @Strain 1.20 %, Temperature 90.0 °C |
6853 psi @Strain 1.20 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 | |
| 48.84 MPa @Strain 1.48 %, Temperature 150 °C |
7084 psi @Strain 1.48 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 51.17 MPa @Strain 2.07 %, Temperature 150 °C |
7422 psi @Strain 2.07 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 | |
| 53.63 MPa @Strain 0.490 %, Temperature -20.0 °C |
7778 psi @Strain 0.490 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 | |
| 55.7 MPa @Strain 0.610 %, Temperature 0.000 °C |
8080 psi @Strain 0.610 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 | |
| 57.58 MPa @Strain 0.590 %, Temperature 40.0 °C |
8351 psi @Strain 0.590 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| 59.43 MPa @Strain 2.86 %, Temperature 150 °C |
8620 psi @Strain 2.86 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 | |
| 64.21 MPa @Strain 1.48 %, Temperature 90.0 °C |
9313 psi @Strain 1.48 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 | |
| 64.53 MPa @Strain 2.39 %, Temperature 150 °C |
9359 psi @Strain 2.39 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 65.31 MPa @Strain 1.97 %, Temperature 90.0 °C |
9472 psi @Strain 1.97 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 | |
| 65.53 MPa @Strain 1.32 %, Temperature 40.0 °C |
9504 psi @Strain 1.32 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 67.63 MPa @Strain 0.640 %, Temperature -20.0 °C |
9809 psi @Strain 0.640 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 | |
| 69.45 MPa @Strain 0.670 %, Temperature 0.000 °C |
10070 psi @Strain 0.670 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 69.61 MPa @Strain 1.25 %, Temperature 23.0 °C |
10100 psi @Strain 1.25 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 | |
| 75.35 MPa @Strain 3.32 %, Temperature 150 °C |
10930 psi @Strain 3.32 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 77.54 MPa @Strain 2.78 %, Temperature 90.0 °C |
11250 psi @Strain 2.78 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 | |
| 80.8 MPa @Strain 0.822 %, Temperature 23.0 °C |
11700 psi @Strain 0.822 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 85.96 MPa @Strain 2.33 %, Temperature 90.0 °C |
12470 psi @Strain 2.33 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 | |
| 86.61 MPa @Strain 2.02 %, Temperature 40.0 °C |
12560 psi @Strain 2.02 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 89.5 MPa @Strain 6.72 %, Temperature 150 °C |
13000 psi @Strain 6.72 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 95.98 MPa @Strain 1.99 %, Temperature 23.0 °C |
13920 psi @Strain 1.99 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 | |
| 101.06 MPa @Strain 3.14 %, Temperature 90.0 °C |
14658 psi @Strain 3.14 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 | |
| 101.42 MPa @Strain 2.71 %, Temperature 40.0 °C |
14710 psi @Strain 2.71 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 109.93 MPa @Strain 1.40 %, Temperature 0.000 °C |
15944 psi @Strain 1.40 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 | |
| 114.76 MPa @Strain 2.74 %, Temperature 23.0 °C |
16645 psi @Strain 2.74 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 | |
| 115.13 MPa @Strain 1.31 %, Temperature 40.0 °C |
16698 psi @Strain 1.31 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| 118.45 MPa @Strain 1.19 %, Temperature 0.000 °C |
17180 psi @Strain 1.19 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 134.55 MPa @Strain 1.91 %, Temperature 0.000 °C |
19515 psi @Strain 1.91 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 | |
| 136.97 MPa @Strain 1.44 %, Temperature -20.0 °C |
19866 psi @Strain 1.44 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 | |
| 138.77 MPa @Strain 1.72 %, Temperature 40.0 °C |
20127 psi @Strain 1.72 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| 146.75 MPa @Strain 1.63 %, Temperature 23.0 °C |
21284 psi @Strain 1.63 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 154.33 MPa @Strain 2.44 %, Temperature 0.000 °C |
22384 psi @Strain 2.44 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 | |
| 157.07 MPa @Strain 1.70 %, Temperature 0.000 °C |
22781 psi @Strain 1.70 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 160.1 MPa @Strain 2.23 %, Temperature 40.0 °C |
23220 psi @Strain 2.23 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| 167.61 MPa @Strain 1.93 %, Temperature -20.0 °C |
24310 psi @Strain 1.93 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 | |
| 173.95 MPa @Strain 2.08 %, Temperature 23.0 °C |
25229 psi @Strain 2.08 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 174.6 MPa @Strain 1.84 %, Temperature -20.0 °C |
25320 psi @Strain 1.84 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 | |
| 183.67 MPa @Strain 2.11 %, Temperature 0.000 °C |
26639 psi @Strain 2.11 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 | |
| 190.98 MPa @Strain 2.43 %, Temperature -20.0 °C |
27699 psi @Strain 2.43 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 | |
| 197.12 MPa @Strain 2.61 %, Temperature 23.0 °C |
28590 psi @Strain 2.61 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 203.2 MPa @Strain 2.28 %, Temperature -20.0 °C |
29470 psi @Strain 2.28 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 | |
| 237.16 MPa @Strain 2.92 %, Temperature -20.0 °C |
34397 psi @Strain 2.92 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |