Karina 809-36/467-CRM Brown PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 809-36/467-CRM Brown PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.33 - 1.39 g/cc
1.33 - 1.39 g/cc
ASTM D 792
ASTM Color 4.94 - 7.94
4.94 - 7.94
Color A, ME 12
12.71 - 15.71
12.71 - 15.71
Color B, ME 12
55.05 - 58.05
55.05 - 58.05
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Elongation at Break >= 5.0 %
>= 5.0 %
ASTM D 638
Descriptive Properties Value Comments
Application Fittings