Polymer Property : Specific Gravity = 1.06 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Mixed 1:1; TM R050-16
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Network Polymers Softflex® 7000
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Specific Gravity 1.06 g/cc
1.06 g/cc
Radici Radilon® S USZ200 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Specific Gravity 1.06 g/cc
1.06 g/cc
ISO 1183
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance
Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide..
Specific Gravity 1.06 g/cc
1.06 g/cc
Momentive Performance Materials Siloprenâ„¢ Electro 242-1 Electrically Insulating Liquid Silicone Rubber
This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate..
Specific Gravity 1.06 g/cc
1.06 g/cc
ISO 1183
Gromax ATE70-FN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Samsung Cheil Industries Starex® WR-9120 ASA, Unreinforced
Information provided by Samsung Cheil Industries.
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Samsung Cheil Industries Starex® WR-9100SG ASA, Unreinforced
Used for solid vinyl door, frame etc.Information provided by Samsung Cheil Industries.
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
SABIC Innovative Plastics NORYL INT2002 PPE+HIPS (Asia Pacific)
PPE/HIPS unfilled for auto interior
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
SABIC Innovative Plastics NORYL PX1265 PPE+PS
Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL.
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
SABIC Innovative Plastics NORYL PX1736 PPE+PS
Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica..
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow 2057E Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 2057E is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2057E is h..
Specific Gravity 1.06 g/cc
1.06 g/cc
Zeon Chemicals Sivic® Z702 Polyblend Nitrile Elastomer
Sivic Z702 is a fully fluxed polyblend of 23% ACN NBR/PVC (70/30). It is produced via a mechanical technology, which provides a lump-free homogenous polymer.Lowest ACN content for improved cold flex..
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
A. Schulman POLYBATCH™ Hot Pink 50377 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 50377 is a hot pink color concentrate based in polyethylene. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 50377 is ty..
Specific Gravity 1.06 g/cc
1.06 g/cc
Trelleborg R483 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Lubrizol Estane® 58123 Thermoplastic Polyurethane
Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack..
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el..
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Lubrizol ESTAGRIP® ST80A Polyether-Type Thermoplastic Polyurethane
Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided..
Specific Gravity 1.06 g/cc
1.06 g/cc
15/15°C
ChevronTexaco Extender
750,000 miles on-road use (8 years or 15,000 hours off-highway use) on initial fill with no Extender neededAdditional Extended service life of 1,000,000 miles/20,000 hours/8 years with Extender adde..
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Denka MALECCA K-200 ABS
A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de..
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Denka MALECCA K-300 ABS
A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de..
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Diamond Polymers ABS 1000
Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc.
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Diamond Polymers ABS 4502
Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc.
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Cheng Yu Plastic A701BK Electric Conducting ABS
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D 792
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP
SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973.
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
SABIC Innovative Plastics NORYL PX2622 PPE+HIPS (Asia Pacific)
PPE/HIPS for auto interior