Polymer Property : Vicat Softening Point = 219 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 104 °C
219 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Vicat Softening Point 104 °C
219 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East)
Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by ..
Vicat Softening Point 104 °C
219 °F
ISO 306/A50
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound
PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS..
Vicat Softening Point 104 °C
219 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications
Vicat Softening Point 104 °C
219 °F
Rate B/50; ISO 306
SABIC Innovative Plastics GELOY XP4025 ASA (Europe-Africa-Middle East)
GELOY XP4025 is a high heat modified ASA/PC blend, for automotive exterior applications. It shows very good properties, gloss and colour retention, as well as faster cycle time over competitive mate..
Vicat Softening Point 104 °C
219 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East)
Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Ravago Manufacturing Americas Hybrid S493 ABS + Polycarbonate Alloy
Medium Impact, Enhanced Heat PerformanceEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin fa..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Total 819E Polystyrene  (discontinued **)
Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Ineos Nova 1511 High Heat Crystal Polystyrene  (discontinued **)
High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Ineos Nova 4214 Medium Impact Polystyrene  (discontinued **)
Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o..
Vicat Softening Point 104 °C
219 °F
Rate B; ASTM D1525
Ineos ABS Lustran® 743 General Purpose, High-Impact  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Vicat Softening Point 104 °C
219 °F
(50 °C/h / 50N) - B/50; ISO 306
Styrolution Luran® S 778 T ASA
Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Vicat Softening Point 104 °C
219 °F
B/50; ISO R306
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Vicat Softening Point 104 °C
219 °F
B/50; ISO R306
Samsung Cheil Industries Starex® SR-0310FM ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Videolar 585 Crystal Polystyrene (GPPS)
High heat extrusion crystalSuperior oriented polystyrene sheetFeatures: Low melt flowHigh molecular weightApplications: Foam applications such as egg cartons, meat trays and food serviceSuperior ori..
Vicat Softening Point 104 °C
219 °F
Conditioned 4 hours @ 70°C (158°F); ASTM D1525
Eastman Tenite Butyrate 285A2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Vicat Softening Point 104 °C

@Load 1.00 kg,
Thickness 3.17 mm
219 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Diamond Polymers ABS 3501 Natural 1002 ESCR Injection Molding Grade, Environmental Stress Crack Resistant
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Vicat Softening Point 104 °C
219 °F
ASTM D1525
C.O.I.M. LARIPUR® LPR5450 Modified Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Americas Styrenics STYRON A-TECH® 1170 High Impact Polystyrene
Product CharacteristicsGood impact resistanceConsistent colorabilityEasy processingFood Contact CompliantUL Classification 94HBTypical ApplicationsExtruded SheetSmall AppliancesRefrigeration Accesso..
Vicat Softening Point 104 °C
219 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron HI-40 B ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Vicat Softening Point 104 °C
219 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Vicat Softening Point 104 °C
219 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Vicat Softening Point 104 °C
219 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Vicat Softening Point 104 °C
219 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Vicat Softening Point 104 °C
219 °F
50°C/hr; 50N
Arkema Group Oroglas® V 825 HID Acrylic, UV, Heat Resistant  (discontinued **)
OROGLAS HID is an acrylic resin formulated to withstand continuous exposure to high intensity discharge ( HID ) sources up to 90°c.Above 80°c, OROGLAS V 825 HID resin retains its original appearan..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Styrolution NAS® 30 Series High Performance Styrenic
It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class..
Vicat Softening Point 104 °C
219 °F
0.125 inch, 1 Kg; ASTM D1525
Diamond Polymers ABS 2510
Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc.