| Category | Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Stanyl® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Stanyl® TW241B3 PA46-CF15.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | dry; ISO 1183 |
| Moisture Absorption | 3.15 % | 3.15 % | Sim. To ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 110 MPa | 16000 psi | cond; ISO 527-1/-2 |
| 185 MPa | 26800 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 2.0 % | 2.0 % | dry; ISO 527-1/-2 |
| 4.0 % | 4.0 % | cond; ISO 527-1/-2 | |
| Tensile Modulus | 13.0 GPa | 1890 ksi | dry; ISO 527-1/-2 |
| Flexural Modulus | 5.80 GPa | 841 ksi | cond; ISO 178 |
| 10.5 GPa | 1520 ksi | dry; ISO 178 | |
| Izod Impact Resistance | 0.450 J/cm² <br>@Temperature -40.0 °C |
2.14 ft-lb/in² <br>@Temperature -40.0 °F |
cond; ISO 180/1A |
| 0.450 J/cm² <br>@Temperature -40.0 °C |
2.14 ft-lb/in² <br>@Temperature -40.0 °F |
dry; ISO 180/1A | |
| 0.500 J/cm² <br>@Temperature 23.0 °C |
2.38 ft-lb/in² <br>@Temperature 73.4 °F |
dry; ISO 180/1A | |
| 1.20 J/cm² <br>@Temperature 23.0 °C |
5.71 ft-lb/in² <br>@Temperature 73.4 °F |
cond; ISO 180/1A | |
| Charpy Impact Unnotched | 4.00 J/cm² <br>@Temperature -30.0 °C |
19.0 ft-lb/in² <br>@Temperature -22.0 °F |
cond; ISO 179/1eU |
| 4.00 J/cm² <br>@Temperature -30.0 °C |
19.0 ft-lb/in² <br>@Temperature -22.0 °F |
dry; ISO 179/1eU | |
| 4.50 J/cm² <br>@Temperature 23.0 °C |
21.4 ft-lb/in² <br>@Temperature 73.4 °F |
dry; ISO 179/1eU | |
| 7.00 J/cm² <br>@Temperature 23.0 °C |
33.3 ft-lb/in² <br>@Temperature 73.4 °F |
cond; ISO 179/1eU | |
| Charpy Impact, Notched | 0.450 J/cm² <br>@Temperature -30.0 °C |
2.14 ft-lb/in² <br>@Temperature -22.0 °F |
cond; ISO 179/1eA |
| 0.450 J/cm² <br>@Temperature -30.0 °C |
2.14 ft-lb/in² <br>@Temperature -22.0 °F |
dry; ISO 179/1eA | |
| 0.500 J/cm² <br>@Temperature 23.0 °C |
2.38 ft-lb/in² <br>@Temperature 73.4 °F |
dry; ISO 179/1eA | |
| 1.20 J/cm² <br>@Temperature 23.0 °C |
5.71 ft-lb/in² <br>@Temperature 73.4 °F |
cond; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | dry; ISO 11359-1/-2 |
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |