Material Notes:
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnification reveals them to be near perfect spheres.PropertiesHigh temperature resistanceGood density/strength ratiosClean surface chemistryNarrow particle size distributionLow thermal conductivityLow dielectric constantLow dissipation factorThe FTD series are washed to remove surface salts, this results in an ideal surface topography for resins or surface treatments to key. The clean ion exchanged surface ensures compatibility with almost any resin system and in particular this series is recommended for sulphur sensitive systems.All information provided by Trelleborg Emerson & Cuming
Physical Properties Metric English Comments
Pellet Density 0.230 - 0.270 g/cc
0.00831 - 0.00975 lb/in³
ASTM D2840
Particle Size 55 µm
55 µm
TEC QSD
pH 6.5 - 9.0
6.5 - 9.0
ASTM D4876
Mechanical Properties Metric English Comments
Modulus of Elasticity 62.0 GPa

@Temperature 25.0 °C
8990 ksi

@Temperature 77.0 °F
62.0 GPa

@Temperature 25.0 °C
8990 ksi

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Softening Point 700 °C
1290 °F
ASTM E794
Optical Properties Metric English Comments
Refractive Index 1.448

@Wavelength 1500 nm
1.448

@Wavelength 1500 nm
1.458

@Wavelength 589.3 nm
1.458

@Wavelength 589.3 nm
Electrical Properties Metric English Comments
Dielectric Constant 1.36 - 1.63

@Frequency 1e+8 Hz
1.36 - 1.63

@Frequency 1e+8 Hz
ASTM D150
Dissipation Factor 0.00050

@Frequency 1.00e+6 - 8.60e+9 Hz
0.00050

@Frequency 1.00e+6 - 8.60e+9 Hz
ASTM D150
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
TED QSD
Descriptive Properties Value Comments
Floatation (% bulk volume) 98
TEC QSD
Isostatic Collapse Pressure, Min. 80% Survival (psi) 1200
ASTM D3102
Packing Factor (min) 62