| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Bead Filled | 
| Manufacturer | CP-Polymer-Technik GmbH & Co. | 
| Trade Name | Wellamid® | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | CP-Polymer-Technik Wellamid® 6000 GS 20 HWCP 20% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 | 
| Moisture Absorption at Equilibrium | 2.0 - 2.5 % | 2.0 - 2.5 % | 23°C/50%RH; DIN 53495 | 
| Linear Mold Shrinkage |           0.0080 - 0.010           cm/cm           @Thickness 4.00 mm  | 
                  0.0080 - 0.010           in/in           @Thickness 0.157 in  | 
        
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength at Break | 75.0 MPa | 10900 psi | 5 mm/min; ISO 527 | 
| Elongation at Break | 8.5 % | 8.5 % | 5 mm/min; ISO 527 | 
| Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 | 
| Flexural Modulus | 3.50 GPa | 508 ksi | DIN 52457 | 
| Charpy Impact Unnotched |           2.50           J/cm²           @Temperature 23.0 °C  | 
                  11.9           ft-lb/in²           @Temperature 73.4 °F  | 
        ISO 179 | 
| Charpy Impact, Notched |           0.600           J/cm²           @Temperature 23.0 °C  | 
                  2.86           ft-lb/in²           @Temperature 73.4 °F  | 
        ISO 179 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear |           65.0           µm/m-°C           @Temperature 23.0 - 80.0 °C  | 
                  36.1           µin/in-°F           @Temperature 73.4 - 176 °F  | 
        DIN 53752 | 
| Melting Point | 215 °C | 419 °F | Kofler | 
| Deflection Temperature at 0.46 MPa (66 psi) | 170 °C | 338 °F | ISO 179 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | ISO 179 | 
| Vicat Softening Point | 200 °C | 392 °F | 50 N; ISO 306 | 
| Flammability, UL94 |           HB                     @Thickness 1.60 mm  | 
                  HB                     @Thickness 0.0630 in  | 
        Stufe; IEC 707 | 
|           HB                     @Thickness 3.20 mm  | 
                  HB                     @Thickness 0.126 in  | 
        Stufe; IEC 707 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 93 | 
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | ISO 3915 | 
| Dielectric Constant |           4.0                     @Frequency 1e+6 Hz  | 
                  4.0                     @Frequency 1e+6 Hz  | 
        IEC 250 | 
| Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 | 
| Dielectric Loss Index | 0.020 | 0.020 | At 1 MHz; IEC 250 | 
| Comparative Tracking Index | 450 V | 450 V | Stufe; IEC 112 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Back Pressure | Low | |
| Holding Pressure | High | |
| Injection Speed | Medium | |
| Screw Speed | High |