Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | |
Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
Water Absorption | 0.80 % | 0.80 % | Saturation; ISO 62 |
Moisture Absorption at Equilibrium | 0.20 % | 0.20 % | 23°C; 50% RH; ISO 62 |
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 2577 |
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
Melt Flow | 58.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
58.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 150 MPa @Load 36.5 kg, Time 30.0 sec |
21800 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Tensile Strength, Yield | 65.0 MPa | 9430 psi | 50 mm/min; ISO 527-2 |
Elongation at Break | 20 % | 20 % | Nominal, 50mm/min; ISO 527-2 |
Elongation at Yield | 7.0 % | 7.0 % | ISO 527-2 |
Modulus of Elasticity | 2.80 GPa | 406 ksi | ISO 527-2 |
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU | |
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA | |
Tensile Creep Modulus, 1000 hours | 1350 MPa | 196000 psi | ISO 899-1 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
Melting Point | 166 °C | 331 °F | DIN 53765 |
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | ISO 75-2 |
Vicat Softening Point | 150 °C | 302 °F | ISO 306 |
Decomposition Temperature | >= 240 °C | >= 464 °F | |
Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Dielectric Constant | 3.8 @Frequency 1.00e+6 Hz |
3.8 @Frequency 1.00e+6 Hz |
IEC 60250 |
3.8 @Frequency 100 Hz |
3.8 @Frequency 100 Hz |
IEC 60250 | |
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
Dissipation Factor | 0.0010 @Frequency 100 Hz |
0.0010 @Frequency 100 Hz |
IEC 60250 |
0.0050 @Frequency 1.00e+6 Hz |
0.0050 @Frequency 1.00e+6 Hz |
IEC 60250 | |
Comparative Tracking Index | 600 V | 600 V | Test solution A; IEC 60112 |
600 V | 600 V | Test solution B; IEC 60112 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 200 °C | 392 °F | Hopper Throat |
Zone 1 | 200 °C | 392 °F | Feed zone |
Zone 2 | 200 °C | 392 °F | Compression |
Zone 3 | 200 °C | 392 °F | Metering-zone |
Zone 4 | 200 °C | 392 °F | Nozzle |
Melt Temperature | 200 °C | 392 °F | Optimal |
190 - 230 °C | 374 - 446 °F | Injection-molding | |
Mold Temperature | 60.0 - 120 °C | 140 - 248 °F | Injection-molding |
90.0 °C | 194 °F | Optimal | |
Drying Temperature | 100 °C | 212 °F | |
Dry Time | 3 hour | 3 hour |
Descriptive Properties | Value | Comments |
---|---|---|
Commercial Status | Europe | |
Ignition Temperature | 320 - 340°C | ASTM D1929 |
Peripheral screw speed | <0.3 m/s | |
Primary Processing Technique | Injection Molding |