Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 2 = 200 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 200 - 210 °C
392 - 410 °F
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp..
Zone 2 200 °C
392 °F
Die
Premix Thermoplastics PRE-ELEC® ESD 6010 Dissipative Masterbatch, IDP Additive
PRE-ELEC® ESD 6010 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro..
Zone 2 200 °C
392 °F
Die
Premix Thermoplastics PRE-ELEC® ESD 6020 Dissipative Masterbatch, IDP Additive
PRE-ELEC® ESD 6020 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro..
Zone 2 200 °C
392 °F
Die
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be..
Zone 2 200 - 230 °C
392 - 446 °F
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro..
Zone 2 200 - 220 °C
392 - 428 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1055D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 2 200 - 220 °C
392 - 428 °F
Extrusion Molding
LG Chemical LI933 Co-Extrusion ASA
Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical
Zone 2 200 - 220 °C
392 - 428 °F
Extrusion Molding
LG Chemical LI970 Co-Extrusion ASA
Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical
Zone 2 200 - 230 °C
392 - 446 °F
Extrusion Molding
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Zone 2 200 - 210 °C
392 - 410 °F
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane
Pearlbondâ„¢ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo..
Zone 2 200 - 230 °C
392 - 446 °F
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as..
Zone 2 200 °C
392 °F
Lubrizol Advanced Materials Pearlthane® ECO D12T80 Thermoplastic Polyurethane
Type : Pearlthane® ECO D12T80 is a high performance bio-based thermoplastic polyurethane. With ca. 42% bio-based content.Main Application : Injection MouldingSpecial Features : Properties similar..
Zone 2 200 °C
392 °F
Injection Molding
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Zone 2 200 - 230 °C
392 - 446 °F
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)
TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist..
Zone 2 200 - 250 °C
392 - 482 °F
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC)
TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products ..
Zone 2 200 - 210 °C
392 - 410 °F
Injection
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane
Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 2 200 - 210 °C
392 - 410 °F
Injection
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
Zone 2 200 °C
392 °F
Extrusion
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Zone 2 200 °C
392 °F
Extrusion
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer
Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Zone 2 200 °C
392 °F
Extrusion
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer
Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Zone 2 200 °C
392 °F
Compression
BASF Ultraform® N2640 E4 POM
Description: Is a POM + MBS, elastomer-modified injection-molding grade with high toughness and high weld line strength.Information provided by BASF
Zone 2 200 °C
392 °F
Compression
BASF Ultraform® N2640 Z2 POM + PUR
Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS..
Zone 2 200 °C
392 °F
Compression
BASF Ultraform® N2770 K POM
Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF
Zone 2 200 °C
392 °F
Compression
BASF Ultraform® S2320 0035 LEV POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF
Zone 2 200 °C
392 °F
Compression
BASF Ultraform® W2320 003 PRO POM
Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF
Zone 2 200 °C
392 °F
Compression
BASF Ultraform® S2320 003 POM
Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF
Zone 2 200 °C
392 °F
Compression
BASF Ultraform® W2320 0035 POM
Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF
Zone 2 200 °C
392 °F
Compression
BASF Ultraform® N2520 XL2 POM
Description: Is a POM, injection-molding grade with increased electrical conductivity, for applications with reduced mechanical requirements.Information provided by BASF
Zone 2 200 - 210 °C
392 - 410 °F
Injection
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane
Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E..
Zone 2 200 °C
392 °F
Compression
BASF Ultraform® N2644 Z9 POM + PUR
Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF
Copyright © lookpolymers.com All Rights Reserved