Arlon 51986XA015 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arlon 51986XA015 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Gray silicone gum and rubber on fiberglass clothThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 63.5 microns
2.50 mil
Side 1; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Interleave
140 microns
5.50 mil
Side 2; Arlon SQA-TMS-003
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
406 microns
16.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
Silicone Property; ASTM D2240
Tensile Strength 5.78 MPa
838 psi
Silicone Property; ASTM D412
Elongation at Break 128 %
128 %
Silicone Property; ASTM D412
Tear Strength 15.6 kN/m
89.0 pli
[ppiw], Die B, Silicone Property; ASTM D624
Peel Strength 0.578 kN/m
3.30 pli
(S2 to S2), Bond Strength; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 28.1 kV/mm
713 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
5.00 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.0833 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Natural
Substrate
Red
Total Product Weight (oz/yd2) 18.1
Arlon SQA-TMS-025