| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
|
Arlon 518581R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon A3015-R004-12 0.015" (0.381 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
 
1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film This..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon A4020-C004FR 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 15% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film FAR 25.853 Recognition: Product is des..
|
|||
| Thickness | 203 microns | 8.00 mil | |
|
Hexcel® HexForce™ 5348 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 51044R020 0.020" Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Semi-cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should no..
|
|||
| Thickness | 203 microns | 8.00 mil | substrate; Arlon SQA-TMS-003 |
|
Arlon 51106RB015D Silicone Rubber/Fiberglass Laminate
Interleave 2: 3 mil PE; Side 2: cured silicone rubber; Substrate: 7628 fiberglass; Side 1: uncured silicone rubber, Interleave 1: 3 mil PE
|
|||
| Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
|
Arlon 51393R031 0.031 (0.635 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: 150 Cycles (temperature and time dependent)This data represents typical values for the production material. T..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 51576XC015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Cured Silicone Rubber This data represents typical values for the production mat..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate |
|
Arlon 51580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should not be ..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh..
|
|||
| Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
|
Arlon 51591R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data ..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 51599R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 51629R020 0.020" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil polyLayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production mat..
|
|||
| Thickness | >= 203 microns | >= 8.00 mil | Side 2, Uncured |
|
Arlon 55578XD028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers Appearance: Gray silicone gum and/or rubber on fiberglass clothThis data Represents typical values for the production ma..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassAppearance: Red silicone rubber on fiberglass fabric.This data represents typical values for the product..
|
|||
| Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
|
Arlon P29609R025 0.025" (0.635 mm) Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr..
|
|||
| Thickness | 203 microns | 8.00 mil | overall; Arlon SQA-TMS-003 |
|
Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
|
|||
| Thickness | 203 microns | 8.00 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
|
|||
| Thickness | 203 microns | 8.00 mil | Overall |
|
Arlon Thermabond®-II 99760N008 0.008" (0.203 mm) Unsupported/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Unsupported/Uncured RubberAppearance: White/gray gumAppearance: White/grey gumThis data Represents typical values for the production material. The data should not be used..
|
|||
| Thickness | 203 - 241 microns | 8.00 - 9.50 mil | Overall |
|
Arlon 44571R008A 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place ..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 51103R015 0.0150" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: LDPEThis data represents typical values for the producti..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical ..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 51808R011 0.011" (0.279 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat This data represents typical values for the production ..
|
|||
| Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
|
Arlon 51946C015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of..
|
|||
| Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
|
Arlon R31651R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
|
|||
| Thickness | >= 203 microns | >= 8.00 mil | Side 2, Uncured |
|
Arlon R33089X028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon R35798R013 0.013" (0.330 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 Fiberglass Side 2: Uncured Silicone RubberThis data represents typic..
|
|||
| Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-012 |
|
Arlon T3020-B002-## 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate
0.5 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number...
|
|||
| Thickness | 203 microns | 8.00 mil | Total; ASTM D3752 |
|
3M 5153 PTFE Glass Cloth Tape
3M™ PTFE Glass Cloth Tape 5151 is constructed using (PTFE) polytetra-fluoroethylene impregnated glass cloth and silicone adhesive. This tape is used in many applications requiring high temperature ..
|
|||
| Thickness | 203 microns | 8.00 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier
Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber..
|
|||