| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | >= 63.5 microns | >= 2.50 mil | Side 2 |
|
Arlon 49581R101 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The..
|
|||
| Thickness | 63.5 microns | 2.50 mil | ASTM D3652 |
|
3M 25A25 Co-Extruded Polyethylene Protective Tapes
3M™ Co-Extruded Polyethylene Protective Tape helps provide temporary protection of painted metals, glass and plastics from surface damage, such as scratching, abrading. etc.Information provided by ..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Liner |
|
3M 7741 Polyester Overlaminating Film
3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per..
|
|||
| Thickness | >= 63.5 microns | >= 2.50 mil | Side 1 |
|
Arlon 49581X010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Interleave |
|
Arlon 51599R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Interleave |
|
Arlon 55946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mate..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Interleave |
|
Arlon 56810R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass This data represents typical values for the production material. The data should not be..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Interleave 2 |
|
Arlon 56811B025 0.026" (0.660 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Product Use: Hose and Duct..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Liner |
|
Arlon Thermabond® 51A50X020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 76..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Side 1; Arlon SQA-TMS-003 |
|
Arlon Thermabond® R36211A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primerDesign/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: St..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Side 2; Arlon SQA-TMS-003 |
|
Arlon Thermabond® R36211A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primerDesign/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: St..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Total; ASTM D3652 |
|
3M Scotch® 821 LabelGard™ Film Tape
Scotch® LabelGard™ Film Tape 821 is a lightly tented pink film designed for protecting labels and packaging lists. The synthetic adhesive is designed for easy handling and dispensing with low stat..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-15 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-176 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-186 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-187 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-273 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-37 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7725-17 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7725-89 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Interleave |
|
Arlon 55108R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone RubberSide 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data rep..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Interleave |
|
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Liner |
|
3M FM001 Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-276 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-38 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7725-47 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7725-48 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-88 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Interleave |
|
Arlon R38726R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured SiliconeProduct Use: Flexible heater substrateAppearance: Red colored, high ..
|
|||
| Thickness | 63.5 microns | 2.50 mil | Substrate |
|
Arlon 48576R006 0.0055" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.0015" PolyethyleneSide 1: Uncured RubberSubstrate: Prime Coated 1080 FiberglassSide 2: Uncured RubberThis data represents typical values for the production mater..
|
|||