Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1250 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D638
PolyOne Nymax™ GF 1200 33 Red 31 A Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D638
Oxford Polymers 30GF 30% Glass Fiber Filled Polycarbonate for Injection Molding
30% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers.
Tensile Modulus 8.65 GPa
1250 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Asia Pacific)
LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D638
Solvay Specialty Polymers Veradel® AG-230 Polyethersulfone  (discontinued **)
For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N..
Tensile Modulus 8.64 GPa
1250 ksi
ASTM D638
Plenco 4224 Phenolic, Granular, Transfer Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability characteristics. It is used in electrical and automotive ap..
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527-1,-2
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibersInformation provided by LANXESS.
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527-1,-2
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Modulus 8.60 GPa
1250 ksi
LATI Latiohm 62-08 PD02 G/30 PPA, 30% Glass Fiber Reinforced
Dissipative product based on Polyamide 6 (PA6). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 8.62 GPa
1250 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP EX07305 PEI (Asia Pacific)
Polyetherimide reinforced with Glass fiber and PTFE for use in Burn-in Test Sockets (BiTS) Application
Tensile Modulus 8.60 GPa
1250 ksi
ISO R 527
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 50
Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America..
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU), 30% Glass Fiber
Veradel® 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber
Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D638
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU), 30% Glass Fiber
Veradel® AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Tensile Modulus 8.60 GPa
1250 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific)
PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump ..
Tensile Modulus 8.63 GPa
1250 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC
LNP* Thermocomp* DF006 is a compound based on Polycarbonate resin containing 30% Glass Fiber.
Tensile Modulus 8.60 GPa
1250 ksi
ASTM D638
Plenco 2308 Phenolic, Granular, Injection Molded
PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai..
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D638
Westlake Plastics Zelux® 30% GF Polycarbonate 30% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Tensile Modulus 8.60 GPa
1250 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Tensile Modulus 8.60 GPa
1250 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime..
Tensile Modulus 8.59 GPa
1250 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON ME003S PP
LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized.
Copyright © lookpolymers.com All Rights Reserved