Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled |
Manufacturer | Addiplast |
Trade Name | Addinyl |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Addiplast Addinyl B2 V15 Nylon 6, 15% Glass Filled.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183/A |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 74 | 74 | Conditioned; ISO 868 |
83 | 83 | ISO 868 | |
Tensile Strength at Break | 70.0 MPa | 10200 psi | Conditioned; ISO R 527 |
125 MPa | 18100 psi | ISO R 527 | |
Elongation at Yield | 3.5 % | 3.5 % | ISO R 527 |
6.0 % | 6.0 % | Conditioned; ISO R 527 | |
Modulus of Elasticity | 3.00 GPa | 435 ksi | Conditioned; ISO 178 |
5.00 GPa | 725 ksi | ISO 178 | |
Izod Impact, Notched (ISO) | 7.50 kJ/m² | 3.57 ft-lb/in² | ISO 180/1A |
13.0 kJ/m² | 6.19 ft-lb/in² | Conditioned; ISO 180/1A | |
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179/IeU |
5.50 J/cm² | 26.2 ft-lb/in² | Conditioned; ISO 179/IeU | |
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/IeA |
1.00 J/cm² | 4.76 ft-lb/in² | Conditioned; ISO 179/IeA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 35.0 µm/m-°C | 19.4 µin/in-°F | ASTM E831 |
Melting Point | 220 °C | 428 °F | ISO 3146/C2 |
Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | ISO 75-2/AF |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | Conditioned; CEI 60093 |
1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
Dielectric Strength | 30.0 kV/mm | 762 kV/in | Conditioned; CEI 60243-1 |
33.0 kV/mm | 838 kV/in | CEI 60243-1 | |
Comparative Tracking Index | 550 V | 550 V | CEI 60112/Solution A |