Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Indium Corporation of America > Category : Nonferrous Metal Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
Indium Corp. 4N Commercial Indium Metal Indium Alloy
Indium Corp. 5N Commercial Indium Metal Indium Alloy
Indium Corp. 6N High Purity Indium Metal Indium Alloy
Indium Corp. 6N5 High Purity Indium Metal Indium Alloy
Indium Corp. 6N5WCI High Purity Indium Metal Indium Alloy
Indium Corp. Indalloy 102 Bismuth-Lead-Tin Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 103 Tin-Cadmium Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 105 Bismuth-Lead-Tin Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 113 Tin-Lead Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 118 Tin-Lead Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 126 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 127 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 128 Pure Tin Pure Element Indalloy
Indium Corp. Indalloy 13 Indium Solder Alloy Indium Alloy Indalloy
Indium Corp. Indalloy 132 Tin Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 140 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 141 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 142 Tin-Lead Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 143 Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 144 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 145 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 146 Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 147 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 148 Pure Bismuth Bismuth Alloy Indalloy
Indium Corp. Indalloy 149 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 15 Low Melting Bismuth Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 152 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 153 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 154 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 155 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 156 Tin Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 157 Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 16 Low Melting Bismuth Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 160 Tin Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 160-190 Fusible Bismuth Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 161 Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 163 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 167 Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 168 Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 169 Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 17 Low Melting Bismuth Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 170 Pure Lead Lead Alloy Indalloy
Indium Corp. Indalloy 172 Tin Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 173 Tin Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 175 Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 176 Zinc Solder Alloy Zinc Alloy Indalloy
Indium Corp. Indalloy 177 Gold-Indium Solder Alloy Gold Alloy Indalloy
Indium Corp. Indalloy 179 Silver Solder Alloy Solder/Braze Alloy Indalloy
Indium Corp. Indalloy 191 Aluminum Solder Alloy Solder/Braze Alloy Indalloy
Indium Corp. Indalloy 192 Pure Aluminum Pure Element Indalloy
Indium Corp. Indalloy 193 Silver Solder Alloy Solder/Braze Alloy Indalloy
Indium Corp. Indalloy 194 Gold Solder Alloy Gold Alloy Indalloy
Indium Corp. Indalloy 196 Gold Solder Alloy Gold Alloy Indalloy
Indium Corp. Indalloy 200 Pure Gold Gold Alloy Indalloy
Indium Corp. Indalloy 21 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 210 Tin-Lead Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 212 Ag-Cu-Zn-Cd Solder Alloy Solder/Braze Alloy Indalloy
Indium Corp. Indalloy 213 Tin-Lead Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 215 Silver Solder Alloy Solder/Braze Alloy Indalloy
Indium Corp. Indalloy 217 Silver Solder Alloy Solder/Braze Alloy Indalloy
Indium Corp. Indalloy 217-440 Bismuth-Lead-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 230 Indium-Tin-Lead Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 234 Bismuth-Lead-Tin Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 251 Tin Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 253 Indium Solder Alloy Indium Alloy Indalloy
Indium Corp. Indalloy 257 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 29 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 31 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 32 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 34 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 35 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 36 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 37 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 40 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 41 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 43 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 44 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 47 Bismuth-Lead-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 48 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 50 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 532 Tin Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 63 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 64 Bismuth Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 65 Bismuth-Lead-Tin Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 67 Bismuth-Lead Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 68 Bismuth-Lead-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 69 Bismuth-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 70 Indium-Tin Solder Alloy Tin Alloy Indalloy
Indium Corp. Indalloy 71 Indium-Tin Solder Alloy Indium Alloy Indalloy
Indium Corp. Indalloy 72 Bismuth-Lead-Tin Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 73 Bismuth-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 74 Bismuth-Lead-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 75 Bismuth-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 76 Bismuth-Lead-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 77 Fusible Gallium Alloy Gallium Alloy Indalloy
Indium Corp. Indalloy 78 Bismuth-Lead-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 79 Bismuth-Lead-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 80 Bismuth-Lead-Tin Solder Alloy Bismuth Alloy Indalloy
Indium Corp. Indalloy 81 Bismuth-Lead-Tin Solder Alloy Lead Alloy Indalloy
Indium Corp. Indalloy 83 Bismuth-Lead-Tin Solder Alloy Lead Alloy Indalloy