Indium Corp. Indalloy 67 Bismuth-Lead Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 67 Bismuth-Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 10.4 g/cc
0.376 lb/in³
Thermal Properties Metric English Comments
Melting Point 124 - 126 °C
255 - 259 °F
Solidus 124 °C
255 °F
Liquidus 126 °C
259 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 58 %
58 %
Lead, Pb 42 %
42 %