Indium Corp. Indalloy 44 Bismuth Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 44 Bismuth Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.32 g/cc
0.337 lb/in³
Thermal Properties Metric English Comments
Melting Point 95.0 - 115 °C
203 - 239 °F
Solidus 95.0 °C
203 °F
Liquidus 115 °C
239 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 50 %
50 %
Lead, Pb 25 %
25 %
Tin, Sn 25 %
25 %