| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 9.81 g/cc | 0.354 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Brinell | 15 <br>@Load 4.00 kg |
15 <br>@Load 8.82 lb |
2mm ball |
| Tensile Strength at Break | 37.2 MPa | 5400 psi | |
| Elongation at Break | 135 % | 135 % | % elongation on 5.65 (sq. root Area) gauge length |
| Shear Strength | 2.07 MPa | 300 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Fusion | 34.3 J/g | 14.8 BTU/lb | |
| Specific Heat Capacity | 0.146 J/g-°C | 0.0349 BTU/lb-°F | Solid |
| Melting Point | 71.0 - 88.0 °C | 160 - 190 °F | |
| Solidus | 71.0 °C | 160 °F | |
| Liquidus | 88.0 °C | 190 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Bismuth, Bi | 42.5 % | 42.5 % | |
| Cadmium, Cd | 8.5 % | 8.5 % | |
| Lead, Pb | 37.7 % | 37.7 % | |
| Tin, Sn | 11.3 % | 11.3 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000400 ohm-cm | 0.0000400 ohm-cm |