| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 11.35 g/cc | 0.4100 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Brinell | 4.0 | 4.0 | |
| Tensile Strength at Break | 12.4 MPa | 1800 psi | |
| Elongation at Break | 55 % | 55 % | |
| Modulus of Elasticity | 18.0 GPa | 2610 ksi | |
| Shear Strength | 12.4 MPa | 1800 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 29.0 µm/m-°C @Temperature 20.0 °C |
16.1 µin/in-°F @Temperature 68.0 °F |
|
| Thermal Conductivity | 35.0 W/m-K @Temperature 85.0 °C |
243 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
| Melting Point | 327 °C | 621 °F | |
| Solidus | 327 °C | 621 °F | |
| Liquidus | 327 °C | 621 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Lead, Pb | 100 % | 100 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000220 ohm-cm | 0.0000220 ohm-cm |