Indium Corp. Indalloy 161 Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Indium Corp. Indalloy 161 Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Torch solder, poor corrosion resistanceInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 11.33 g/cc
0.4093 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.3 MPa
4400 psi
Elongation at Break 42 %
42 %
Shear Strength 20.0 MPa
2900 psi
Thermal Properties Metric English Comments
Melting Point 303 °C
577 °F
Eutectic
Solidus 303 °C
577 °F
Liquidus 303 °C
577 °F
Component Elements Properties Metric English Comments
Lead, Pb 97.5 %
97.5 %
Silver, Ag 2.5 %
2.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000200 ohm-cm
0.0000200 ohm-cm