Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. 6N5WCI High Purity Indium Metal

Category Metal , Nonferrous Metal , Indium Alloy , Pure Element
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 6N5WCI High Purity Indium Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High purity Indium is used as the starting material in the manufacture of indium based group III-V such asIn/PIn/AsIn/SbIn/Ga/AsIn/Ga/As/P These compound semiconductors find use in ultra high efficiency photovoltaic solar cells, infrared detectors, infrared LEDs and electronic switching applications where silicon based devices are not suitable.High purity indium is also used as the source material for semiconductor epitaxial layering using liquid phase, vapor phase or molecular beam epitaxy.Total impurities for 6N5 grade < 0.5 ppmThis grade is offered with controlled impurities.Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Component Elements Properties Metric English Comments
Copper, Cu 0.0000050 %
0.0000050 %
Indium, In 99.9999 %
99.9999 %
Iron, Fe 0.000015 %
0.000015 %
Lead, Pb 0.000018 %
0.000018 %
Thallium, Tl 0.0000090 %
0.0000090 %
Tin, Sn 0.000010 %
0.000010 %
Trace Metals <= 0.000020 %
<= 0.000020 %
Total combined metals