Category | Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Pure Element |
Manufacturer | Indium Corporation of America |
Trade Name | Indalloy |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Indium Corp. Indalloy 200 Pure Gold.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 19.3 g/cc | 0.697 lb/in³ |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 138 MPa | 20000 psi | |
Elongation at Break | 39 - 45 % | 39 - 45 % | 2in. |
Modulus of Elasticity | 77.2 GPa | 11200 ksi |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.0 µm/m-°C @Temperature 20.0 °C |
7.78 µin/in-°F @Temperature 68.0 °F |
|
Specific Heat Capacity | 0.130 J/g-°C | 0.0311 BTU/lb-°F | Solid |
Thermal Conductivity | 318 W/m-K @Temperature 85.0 °C |
2210 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Melting Point | 1064 °C | 1947 °F | |
Solidus | 1064 °C | 1947 °F | |
Liquidus | 1064 °C | 1947 °F |
Component Elements Properties | Metric | English | Comments |
---|---|---|---|
Gold, Au | 100 % | 100 % |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000230 ohm-cm | 0.00000230 ohm-cm |