Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | DIN 53 483 |
Perstorp Compounds 371 Urea-Formaldehyde w/ cellulose filler Information provided by Perstorp Compounds Inc. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | C - 96/35/90; IPC-TM-650.2.5.17.1 |
Park Electrochemical Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | |
Covestro Apec® 1600 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | |
Covestro Apec® DP 1-9379/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 93 |
LG Chemical LG-749 ABS, Low Gloss, High Heat Resistance Information Provided by LG Chem |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | d.a.m.; IEC 60093 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 402H1 Natural PA66, Conditioned Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Teijin Panlite® G-3120PH For Cameras, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 30 % of special GF and improved appearance grade.Applications:Precision machinery, electric and electronic components that need dimensional accuracy and good appearance.Information p.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Teijin Panlite® LS-2250 Friction and Abrasion Resistant Polycarbonate Resin It is compounded with fluorine powder to improve friction and abrasion resistance, meeting UL 94 V-2. The friction and abrasion resistance is superior than that of polyamidoacetal, maintaining excel.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 HS MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedTPCI# 9094101Information provided by TP Composites, Inc. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Styrolution Terlux® 2812 HD MABS Description: Terlux 2812 HD is a suitable grade for the food packaging and health care and diagnostic markets.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Bayblend® FR 3008 HR Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and very good hydrolysis resistance antimony-, chlorine- and bromine-free flame.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Bayblend® T65 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Makroblend® KU 2-7912 MBS151 Polycarbonate + PBT, Impact Grade (PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedAs of 1 September 2015, Bayer MaterialScience was separated.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Makrolon® 2556 Polycarbonate MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Makrolon® LED2045 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeMVR (250 °C/2.16 kg) 16.5 cm3/10minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable .. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® L 20 G grey 9280 PA12 Product Description: Grilamid L 20 G grey 9280 is a medium viscosity, unreinforced, heat stabilized polyamide 12 for injection molding and cable sheathing. The main features of this product are: Low.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® LVX-50H black 9230 PA12-GF50 Product description: Grilamid LVX-50H black 9230 is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® LVX-50H nat PA12-GF50 Product description: Grilamid LVX-50H natural is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and st.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® TSG-30/4 H black 9836 PA666-GF30 Information provided by EMS Grivory |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® OE100-T High Temperature Epoxy Material Description: A two component, high Tg, high temperature grade epoxy designed for semiconductor, underfill, hard-disk drive and hybrid micro-electronics packaging applications. The epoxy ca.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
Barlog Plastics KEBAFLOW HF140 LCP, 40% glass fiber reinforced LCP-GF40Information provided by BARLOG plastics GmbH. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
BASF Ultraform S 2320 003 UNC Q600 POM Ultraform S2320 003 UNC Q600 is an easy flowing and rapidly freezing injection molding POM grade. Contains a mold release agent. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |