Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 402H1 Natural PA66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay TECHNYL® A 402H1 Natural PA66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The product offers three main advantages: high impact resistance at low humidity levels, good rigidity, and excellent compression resistance.Available in: Asia Pacific, Europe and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: This grade is particularly suitable for the extrusion of window profiles or semi-finished products, and for the injection molding of plastic insulators for railway binding.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527 type 1 A
Elongation at Break 250 %
250 %
ISO 527 Type 1A
Elongation at Yield 30 %
30 %
ISO 527 type 1 A
Tensile Modulus 1.30 GPa
189 ksi
ISO 527 Type 1A
Flexural Strength 75.0 MPa
10900 psi
ISO 178
Flexural Modulus 1.30 GPa
189 ksi
ISO 178
Izod Impact, Notched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
ISO 180/1eA
Charpy Impact, Notched 3.00 J/cm²
14.3 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243
Dissipation Factor 0.10
0.10
IEC 60250
Comparative Tracking Index 575 V
575 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %