Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | Moist |
Fujipoly Industries FLAT-5TV-20-.75 silicone rubber fusible tape Information provided by Fujipoly Industries |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | Moist |
Fujipoly Industries FLAT-5TV-8-1.0 silicone rubber fusible tape Information provided by Fujipoly Industries |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | ASTM D257 |
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (Conditioned) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | Moist |
Fujipoly Industries DELTA-5TV-20-1 silicone rubber fusible tape Information provided by Fujipoly Industries |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | |
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (Conditioned) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Solvay TECHNYL® C 502XT PA6, Conditioned Description: Unreinforced polyamide 6, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rods, profiles, shee.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY KX01002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX01002 is a compound based on Acetal Copolymer resin containing Antistat. Added features include: Permanent Anti-Static. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | Practical Use (Water Absorption 0.8%); ASTM-D257 |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 100 °C |
1.00e+10 ohm-cm @Temperature 212 °F |
|
Tra-Con Tra-Bond CA20 Coil-Fix Epoxy Adhesive TRA-BOND CA-20 is a thixotropic epoxy adhesive system specially formulated for shorted turns, damaged end wire extensions, or other coil repair applications where a high-fill, non-sag adhesive is re.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Conditioned, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Conditioned, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Thickness 3.00 mm |
1.00e+10 ohm-cm @Thickness 0.118 in |
IEC 60093 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Conditioned) Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | Moist |
Fujipoly Industries FLAT-5TV-20-1 silicone rubber fusible tape Information provided by Fujipoly Industries |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3L PA6 (Conditioned) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Solvay TECHNYL® 1015CR PA6, Conditioned Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Solvay TECHNYL® 1021ST PA6, Conditioned Description: Polyamide 6, unfilled, super tough impact modified, for injection moldingAvailable in: Asia Pacific Product Applications: TECHNYL® 102ST has the highest level impact strength and balan.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Solvay TECHNYL® 2411GF6 PA66, 30% glass fiber, Conditioned Description: Polyamid 66, 30% glass fiber reinforce, for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2411GF6 used in all sectors of industry, offering an excellent com.. |