Solvay TECHNYL® 1021ST PA6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® 1021ST PA6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Polyamide 6, unfilled, super tough impact modified, for injection moldingAvailable in: Asia Pacific Product Applications: TECHNYL® 102ST has the highest level impact strength and balanced mechanical properties. It is suitable for all sectors industries such as: Bowling pin, Brake drum, Inline skate part. This product is available natural colors on request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC60250
Dielectric Strength 18.0 kV/mm
457 kV/in
IEC 60243
Dissipation Factor 0.12
0.12
IEC 60250
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %