Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | VDE 0303 |
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 0177 B Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 CM40 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural .. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Teijin Panlite® GS-3430 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Teijin Panlite® LN-2250Y Flame Resistant, Translucent Polycarbonate Resin Flame retardant and mold release grade with normal fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications.Applications:Electric,.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
Styrolution Terluran® HD-15 ABS Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 HS MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedTPCI# 9094101Information provided by TP Composites, Inc. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | |
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation .. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | ASTM D257 |
Unitika M1030B PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Bayblend® T88-2N Polycarbonate + ABS, 10% Glass Filled Injection molding grade10 % glass fiber filledtensile modulus = 3900 MPaVicat/B 120 temperature = 131 °CPreprocessingMax. Water content |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Makroblend® S 7916/2 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Makrolon® 8315 Polycarbonate, 10% Glass Filled MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityeasy releaseinjection moldingavailable in opaque colors onlyPreprocessingMax. Water content |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Makrolon® AL2447 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minAutomotive lightingLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpa.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® L 20H FWA black 9225 PA12 Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded .. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® TSGL-40/4 FA black 9840 PA666-GF40 Product description: Grilon TSGL-40/4 FA black 9840 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 FA black 9840 is characterized by th.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® 320NC-2 Optically Opaque Epoxy Material Description: A two component, black colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Covestro Makrolon® DP1-1843* Polycarbonate ISO 7391-PC,RL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 9.5 cm3/10 minMedium viscosityUV stabilizedRotomoldingAvailable in transparent and translucent colorsGlobe lightsAs of 1 September 2.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |