EMS-Grivory Grivory® L 25 W 40 NZ PA12-I

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® L 25 W 40 NZ PA12-I.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The main features of Grilamid L 25 W 40 NZ are: Exceptional impact strength, also at low temperaturesFlexibilityUV and heat stabilityLow density, low weightEasy processing Application examples: Grilamid L 25 W 40 NZ is suitable for the production of flexible tubes and profiles requiring good low temperature impact strength for use in automotive and industrial applications.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Water Absorption 1.4 %
1.4 %
ISO 62
Moisture Absorption 0.700 %
0.700 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 25.0 MPa
3630 psi
conditioned; ISO 2039-1
Tensile Strength at Break 30.0 MPa
4350 psi
conditioned; ISO 527-1/-2
45.0 MPa
6530 psi
dry; ISO 527-1/-2
Tensile Strength, Yield 20.0 MPa
2900 psi
conditioned; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
>= 50 %
>= 50 %
dry; ISO 527-1/-2
Elongation at Yield 45 %
45 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.250 GPa
36.3 ksi
conditioned; ISO 527-1/-2
0.300 GPa
43.5 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched NB
NB
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.30 J/cm²

@Temperature 30.0 °C
6.19 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 173 °C
343 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C
176 °F
long term; EMS
110 °C
230 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ISO 75-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Plasticizer
Automotive Compressed air systems
Fuel systems
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Product Attributes Flexible
High viscosity
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)