Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
1.08 g/cc @Temperature 300 °C |
0.0390 lb/in³ @Temperature 572 °F |
Melt | |
Water Absorption | 0.26 % | 0.26 % | Similar to ISO 62 |
Moisture Absorption at Equilibrium | 0.10 % | 0.10 % | Similar to ISO 62 |
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | ISO 294-4,2577 |
Melt Flow | 6.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 50.0 MPa | 7250 psi | ISO 527-1/-2 |
Elongation at Break | 8.5 % | 8.5 % | ISO 527-1/-2 |
Tensile Modulus | 3.90 GPa | 566 ksi | ISO 527-1/-2 |
Impact | 3800 | 3800 | Puncture - maximum force (N); ISO 6603-2 |
3000 @Temperature -30.0 °C |
3000 @Temperature -22.0 °F |
Puncture - maximum force (N); ISO 6603-2 | |
Puncture Energy | 25.0 J | 18.4 ft-lb | ISO 6603-2 |
10.0 J @Temperature -30.0 °C |
7.38 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | Melt |
Thermal Conductivity | 0.191 W/m-K | 1.33 BTU-in/hr-ft²-°F | Melt |
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ISO 75-1/-2 |
Deflection Temperature at 1.8 MPa (264 psi) | 138 °C | 280 °F | ISO 75-1/-2 |
Vicat Softening Point | 147 °C | 297 °F | 50°C/h 50N; ISO 306 |
Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
IEC 60695-11-10 |
V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
IEC 60695-11-10 | |
Oxygen Index | 27 % | 27 % | ISO 4589-1/-2 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
Dielectric Constant | 3.2 @Frequency 100 Hz |
3.2 @Frequency 100 Hz |
IEC 60250 |
3.2 @Frequency 1.00e+6 Hz |
3.2 @Frequency 1.00e+6 Hz |
IEC 60250 | |
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
Dissipation Factor | 0.0010 @Frequency 100 Hz |
0.0010 @Frequency 100 Hz |
IEC 60250 |
0.0090 @Frequency 1.00e+6 Hz |
0.0090 @Frequency 1.00e+6 Hz |
IEC 60250 | |
Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 300 °C | 572 °F | Injection Molding; ISO 294 |
310 - 330 °C | 590 - 626 °F | ||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
110 °C | 230 °F | Injection Molding; ISO 10724 | |
Ejection Temperature | 140 °C | 284 °F | |
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Descriptive Properties | Value | Comments |
---|---|---|
Availability | North America | |
Eff. thermal diffusivity (m²/s) | 1.11E-07 | |
Feature | Release agent | |
Form | Pellets | |
Process | Injection Molding | |
Other Extrusion |