Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Solvay TECHNYL® PSB 286 PA6, Conditioned Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl.. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+11 ohm-cm | 1.00e+10 - 1.00e+11 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI (Asia Pacific) LNP* Thermocomp* ECF62 is a compound based on Polyetherimide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
Techmer ES Statiblend® ABS GF20 AS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PA6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Antistatic, Heat Stabilizer and LubricantFeatures: Antistatic, Heat Stabilizer and Lubricate.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | Practical Use (Water Absorption 1.25%); ASTM-D257 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Temperature 100 °C |
1.00e+10 ohm-cm @Temperature 212 °F |
|
Tra-Con Tra-Bond 2116 Low Vapor Pressure Epoxy Staking Compound TRA-BOND 2116 is a thixotropic, low vapor pressure epoxy system that passes the NASA Outgassing Specification. It is recommended for critical electronic, aerospace, and industrial applications where.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® 2D 20 nat PA612 Product Description: Grilamid 2D 20 natural is an unmodified unreinforced, medium viscosity polyamide 612 (PA612), designed for injection molding as well as extrusion. It is characterized by the fol.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® XE 4188 black 9992 PA612 Product description: Grilamid XE 4188 black 9992 is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 black 9992 are: High v.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | |
Cotronics 4420 One-Part Epoxy |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Conditioned AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Conditioned, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Conditioned, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Conditioned) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Volume Resistivity | 1.00e+10 - 3.16e+10 ohm-cm | 1.00e+10 - 3.16e+10 ohm-cm | IS 3396-1979 |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Conditioned, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Thickness 0.750 mm |
1.00e+10 ohm-cm @Thickness 0.0295 in |
IEC 60093 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned) Ultramid A 3HG2 is a 10% glass fiber reinforced grade of nylon 6/6 for injection molding. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Volume Resistivity | 1.00e+10 ohm-cm @Thickness 0.750 mm |
1.00e+10 ohm-cm @Thickness 0.0295 in |
IEC 60093 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3S BK00464 PA6 (Conditioned) Description: Easy flowing, finely crystalline injection-molding grade for very fast processing. Uses include thin-walled technical parts (eg. housings, fittings, grips, small parts and fixing clamps.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
BASF Ultramid® B3S HP PA6 (Conditioned) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Solvay TECHNYL® 1021GF6 PA6, 30% glass fiber, Conditioned Description: Polyamide 6, 30% glass fiber reinforced, for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 1021GF6 is used in all sectors of industry, offering an excelle.. |
|||
Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
Solvay TECHNYL® 1021ST PA6, Conditioned Description: Polyamide 6, unfilled, super tough impact modified, for injection moldingAvailable in: Asia Pacific Product Applications: TECHNYL® 102ST has the highest level impact strength and balan.. |