Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243 |
Polimeri Europa Edistir RK 451G Polystyrene UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded, high impact polystyrene. This grade combines medium flow, heat resistance and good light stability for injection moulding of technical p.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 2.00 mm |
660 kV/in @Thickness 0.0787 in |
IEC 60243-1 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243 |
Polimeri Europa Edistir RK Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical KEYFLEX BT 1155D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG .. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243 |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243 |
Solvay TECHNYL® A 208F PA66, Conditioned Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243 |
Solvay TECHNYL® A 216 NATURAL FA PA66, Conditioned Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243 |
Solvay TECHNYL® A 216 PA66, Conditioned Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 243 |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | dry; IEC 60243-1 |
DSM Novamid® 1011CH5KR PA6 Heat Stabilized, Easy Molding Grade |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | dry; IEC 60243-1 |
DSM Novamid® 3010SR NAT PA66 Easy Molding Grade |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® TSG-35 PA666-GF35 Information provided by EMS Grivory |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243-1 |
DuPont Performance Polymers Crastin® FG6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6129 NC010 is an unreinforced high viscosity polybutylene.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243-1 |
DuPont Performance Polymers Crastin® FG6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6130 NC010 is an unreinforced medium high viscosity polyb.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | |
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
ASTM D149 |
E-Polymers SEPAZ® C130M 30% Mineral Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 2.00 mm |
660 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® MN301-G0 Nylon 66 Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243 |
Solvay TECHNYL® A 218 S30 Black 21 N PA66, 30% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 30% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 218 S30 is used in all sectors of indu.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | Conditioned; IEC 60243 |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TS V0 PA666 Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous.. |