Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 43.0 kV/mm @Thickness 0.800 mm |
1090 kV/in @Thickness 0.0315 in |
Short Term; ASTM D149 |
Shell Carilon® DB6F0A10 Polyketone, Flame-Retarded (V-0) Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F0A10 is a flame-retarded injection molding grade with mechanical properties which classify it a.. |
|||
Dielectric Strength | 42.91 kV/mm | 1090 kV/in | |
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA) High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® BKV 215 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning .. |
|||
Dielectric Strength | 42.9 kV/mm | 1090 kV/in | ASTM D149 |
LyondellBasell Hifaxâ„¢ AA36H Polypropylene Homopolymer Description: Hifaxâ„¢ AA36H conventional melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabi.. |
|||
Dielectric Strength | 42.9 kV/mm | 1090 kV/in | ASTM D149 |
LyondellBasell Hifaxâ„¢ AA56H Polypropylene Homopolymer Description: Hifaxâ„¢ AA56H medium high melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabil.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 414 Paper, 3.4 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65 Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | IEC 60243-1 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | DAM; IEC 60243-1 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR NC010 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin. It is also a P.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | IEC 60243-1 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | |
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene H 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene H 490 M10S Flame Retardant Polypropylene Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene H 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene H 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene H 490 S Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene H 590 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene J 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene J 490 S Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene J 690 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene PMD 50218 Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Dielectric Strength | 42.9 kV/mm | 1090 kV/in | ASTM D149 |
Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 15 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction:Liner: FEPProduct: Uncured Silicone Rub.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | IEC 60243-1 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | IEC 60243-1 |
BASF Ultraform® N2200 G43 POM Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | IEC 60243-1 |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene J 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | IEC 60243-1 |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTROMID 12 LE soft Polyamide 12 LE soft This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | |
Arkema Group Pebax® MX 1205 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | CEI 60243-1 |
Addiplast Addilene PMD 50203 Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |