Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
Viscosity | 88855 cP @Shear Rate 5000 1/s, Temperature 230 °C |
88855 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
90970 cP @Shear Rate 5000 1/s, Temperature 215 °C |
90970 cP @Shear Rate 5000 1/s, Temperature 419 °F |
ISO 11403-1 -2 | |
99370 cP @Shear Rate 5000 1/s, Temperature 200 °C |
99370 cP @Shear Rate 5000 1/s, Temperature 392 °F |
ISO 11403-1 -2 | |
254390 cP @Shear Rate 500 1/s, Temperature 230 °C |
254390 cP @Shear Rate 500 1/s, Temperature 446 °F |
ISO 11403-1 -2 | |
309200 cP @Shear Rate 500 1/s, Temperature 215 °C |
309200 cP @Shear Rate 500 1/s, Temperature 419 °F |
ISO 11403-1 -2 | |
350800 cP @Shear Rate 500 1/s, Temperature 200 °C |
350800 cP @Shear Rate 500 1/s, Temperature 392 °F |
ISO 11403-1 -2 | |
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 2577 |
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 93 | 93 | ISO 2039-2 |
Hardness, Rockwell R | 121 | 121 | ISO 2039-2 |
Tensile Stress | 5.90 MPa @Strain 0.400 %, Temperature 90.0 °C |
856 psi @Strain 0.400 %, Temperature 194 °F |
ISO 11403-1 -2 |
17.2 MPa @Strain 0.500 %, Temperature 23.0 °C |
2490 psi @Strain 0.500 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
20.5 MPa @Strain 1.70 %, Temperature 90.0 °C |
2970 psi @Strain 1.70 %, Temperature 194 °F |
ISO 11403-1 -2 | |
22.6 MPa @Strain 0.600 %, Temperature 0.000 °C |
3280 psi @Strain 0.600 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
29.1 MPa @Strain 3.00 %, Temperature 90.0 °C |
4220 psi @Strain 3.00 %, Temperature 194 °F |
ISO 11403-1 -2 | |
34.1 MPa @Strain 4.40 %, Temperature 90.0 °C |
4950 psi @Strain 4.40 %, Temperature 194 °F |
ISO 11403-1 -2 | |
40.1 MPa @Strain 1.00 %, Temperature -40.0 °C |
5820 psi @Strain 1.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |
49.9 MPa @Strain 2.10 %, Temperature 23.0 °C |
7240 psi @Strain 2.10 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
62.2 MPa @Strain 3.70 %, Temperature 23.0 °C |
9020 psi @Strain 3.70 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
64.8 MPa @Strain 2.50 %, Temperature 0.000 °C |
9400 psi @Strain 2.50 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
66.4 MPa @Strain 5.00 %, Temperature 23.0 °C |
9630 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
79.0 MPa @Strain 4.50 %, Temperature 0.000 °C |
11500 psi @Strain 4.50 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
83.7 MPa @Strain 7.00 %, Temperature 0.000 °C |
12100 psi @Strain 7.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
90.8 MPa @Strain 4.00 %, Temperature -40.0 °C |
13200 psi @Strain 4.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |
97.8 MPa @Strain 7.00 %, Temperature -40.0 °C |
14200 psi @Strain 7.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |
98.4 MPa @Strain 10.0 %, Temperature -40.0 °C |
14300 psi @Strain 10.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |
Tensile Strength, Yield | 73.5 MPa | 10700 psi | ISO 527-1/-2 |
Elongation at Break | 27 % | 27 % | Nominal; ISO 527-1/-2 |
Elongation at Yield | 13 % | 13 % | ISO 527-1/-2 |
Tensile Modulus | 3.35 GPa | 486 ksi | ISO 527-1/-2 |
Flexural Strength | 85.0 MPa @Strain 3.50 % |
12300 psi @Strain 3.50 % |
ISO 178 |
Flexural Modulus | 3.15 GPa | 457 ksi | ISO 178 |
Secant Modulus | 0.758 GPa @Strain 13.0 %, Temperature -40.0 °C |
110 ksi @Strain 13.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
0.940 GPa @Strain 9.00 %, Temperature 0.000 °C |
136 ksi @Strain 9.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
0.984 GPa @Strain 7.00 %, Temperature 23.0 °C |
143 ksi @Strain 7.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
1.225 GPa @Strain 8.00 %, Temperature -40.0 °C |
177.7 ksi @Strain 8.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |
1.50 GPa @Strain 4.30 %, Temperature 23.0 °C |
218 ksi @Strain 4.30 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
1.612 GPa @Strain 5.00 %, Temperature 0.000 °C |
233.8 ksi @Strain 5.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
2.27 GPa @Strain 4.00 %, Temperature -40.0 °C |
329 ksi @Strain 4.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |
2.38 GPa @Strain 2.10 %, Temperature 23.0 °C |
345 ksi @Strain 2.10 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
2.592 GPa @Strain 2.50 %, Temperature 0.000 °C |
375.9 ksi @Strain 2.50 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
3.44 GPa @Strain 0.500 %, Temperature 23.0 °C |
499 ksi @Strain 0.500 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
3.77 GPa @Strain 0.600 %, Temperature 0.000 °C |
546 ksi @Strain 0.600 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
4.01 GPa @Strain 1.00 %, Temperature -40.0 °C |
582 ksi @Strain 1.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 | |
Charpy Impact Unnotched | 25.0 J/cm² | 119 ft-lb/in² | ISO 179/1eU |
22.5 J/cm² @Temperature -30.0 °C |
107 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU | |
Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179/1eA |
0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | ISO 75-1/-2 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
Dielectric Constant | 3.8 @Frequency 1.00e+6 Hz |
3.8 @Frequency 1.00e+6 Hz |
IEC 60250 |
3.9 @Frequency 100 Hz |
3.9 @Frequency 100 Hz |
IEC 60250 | |
Dielectric Strength | 43.0 kV/mm | 1090 kV/in | IEC 60243-1 |
Dissipation Factor | 0.00050 @Frequency 100 Hz |
0.00050 @Frequency 100 Hz |
IEC 60250 |
0.0055 @Frequency 1.00e+6 Hz |
0.0055 @Frequency 1.00e+6 Hz |
IEC 60250 | |
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Descriptive Properties | Value | Comments |
---|---|---|
Delivery Form | Pellets | |
Emissions | <2 mg/kg | VDA 275 |
Part Marking Code | >POM< | ISO 11469 |
Processing | Injection Moulding | |
Regional Availability | Asia Pacific | |
Europe | ||
Global | ||
Near East/Africa | ||
North America | ||
South and Central America | ||
Resin Identification | POM | ISO 1043 |