Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very .. |
|||
Dielectric Strength | 23.0 - 35.0 kV/mm | 584 - 889 kV/in | IEC 60243-1 |
Raschig Group RALUPOL® 4385 UP Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Dielectric Strength | 18.0 - 35.0 kV/mm | 457 - 889 kV/in | Average value: 25.0 kV/mm Grade Count:54 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Dielectric Strength | 16.1 - 35.0 kV/mm | 409 - 889 kV/in | Average value: 25.6 kV/mm Grade Count:6 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Dielectric Strength | 15.7 - 35.0 kV/mm | 400 - 889 kV/in | Average value: 21.3 kV/mm Grade Count:25 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Dielectric Strength | 15.0 - 35.0 kV/mm | 380 - 889 kV/in | Average value: 28.4 kV/mm Grade Count:20 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Dielectric Strength | 16.0 - 35.0 kV/mm | 406 - 889 kV/in | Average value: 29.1 kV/mm Grade Count:29 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Dielectric Strength | 14.9 - 35.0 kV/mm | 378 - 889 kV/in | Average value: 24.6 kV/mm Grade Count:69 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Dielectric Strength | 15.7 - 35.0 kV/mm | 400 - 889 kV/in | Average value: 27.6 kV/mm Grade Count:10 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Dielectric Strength | 8.60 - 35.0 kV/mm | 218 - 889 kV/in | Average value: 17.7 kV/mm Grade Count:20 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Dielectric Strength | 19.7 - 35.0 kV/mm | 500 - 889 kV/in | Average value: 24.6 kV/mm Grade Count:18 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Dielectric Strength | 19.0 - 35.0 kV/mm | 483 - 889 kV/in | Average value: 26.6 kV/mm Grade Count:12 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | Average value: 29.2 kV/mm Grade Count:6 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Dielectric Strength | 21.0 - 35.0 kV/mm | 533 - 889 kV/in | Average value: 27.5 kV/mm Grade Count:4 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Dielectric Strength | 20.0 - 35.0 kV/mm | 508 - 889 kV/in | Average value: 26.0 kV/mm Grade Count:40 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Dielectric Strength | 30.0 - 35.0 kV/mm | 762 - 889 kV/in | Average value: 32.0 kV/mm Grade Count:12 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |
|||
Dielectric Strength | 30.0 - 35.0 kV/mm | 762 - 889 kV/in | DIN 53481 |
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | 17.7 - 35.0 kV/mm | 450 - 889 kV/in | Average value: 23.9 kV/mm Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Dielectric Strength | 32.0 - 35.0 kV/mm | 813 - 889 kV/in | Average value: 33.7 kV/mm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |