Overview of materials for Polycarbonate, Impact Modified

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Impact Modified
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polycarbonate, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.02 - 1.43 g/cc
0.0368 - 0.0517 lb/in³
Average value: 1.20 g/cc Grade Count:86
1.02 - 1.02 g/cc

@Temperature 280 - 300 °C
0.0368 - 0.0368 lb/in³

@Temperature 536 - 572 °F
Average value: 1.02 g/cc Grade Count:6
Water Absorption 0.0900 - 0.400 %
0.0900 - 0.400 %
Average value: 0.236 % Grade Count:23
Moisture Absorption at Equilibrium 0.120 - 0.340 %
0.120 - 0.340 %
Average value: 0.161 % Grade Count:21
Water Absorption at Saturation 0.300 - 0.500 %
0.300 - 0.500 %
Average value: 0.361 % Grade Count:9
Viscosity 360000 - 380000 cP

@Temperature 260 - 260 °C
360000 - 380000 cP

@Temperature 500 - 500 °F
Average value: 370000 cP Grade Count:2
360000 - 380000 cP

@Shear Rate 1000 - 1000 1/s
360000 - 380000 cP

@Shear Rate 1000 - 1000 1/s
Average value: 370000 cP Grade Count:2
Maximum Moisture Content 0.0200 - 0.0400
0.0200 - 0.0400
Average value: 0.0213 Grade Count:15
Linear Mold Shrinkage 0.00100 - 0.0300 cm/cm
0.00100 - 0.0300 in/in
Average value: 0.00641 cm/cm Grade Count:75
Linear Mold Shrinkage, Transverse 0.00300 - 0.0100 cm/cm
0.00300 - 0.0100 in/in
Average value: 0.00668 cm/cm Grade Count:19
Melt Flow 3.30 - 35.0 g/10 min
3.30 - 35.0 g/10 min
Average value: 14.6 g/10 min Grade Count:68
Mechanical Properties Metric English Comments
Hardness, Rockwell L 70.0 - 89.0
70.0 - 89.0
Average value: 82.7 Grade Count:3
Hardness, Rockwell R 111 - 122
111 - 122
Average value: 117 Grade Count:31
Ball Indentation Hardness 113 MPa
16400 psi
Average value: 113 MPa Grade Count:4
Tensile Strength, Ultimate 50.0 - 228 MPa
7250 - 33000 psi
Average value: 68.5 MPa Grade Count:33
Tensile Strength, Yield 51.0 - 138 MPa
7400 - 20000 psi
Average value: 61.5 MPa Grade Count:74
Elongation at Break 2.00 - 130 %
2.00 - 130 %
Average value: 77.1 % Grade Count:66
Elongation at Yield 4.00 - 90.0 %
4.00 - 90.0 %
Average value: 12.2 % Grade Count:29
Modulus of Elasticity 0.225 - 3.95 GPa
32.6 - 573 ksi
Average value: 2.28 GPa Grade Count:28
Flexural Yield Strength 68.9 - 179 MPa
10000 - 26000 psi
Average value: 91.2 MPa Grade Count:63
Flexural Modulus 1.91 - 8.27 GPa
277 - 1200 ksi
Average value: 2.54 GPa Grade Count:66
Izod Impact, Notched 0.785 - 9.08 J/cm
1.47 - 17.0 ft-lb/in
Average value: 5.97 J/cm Grade Count:64
3.74 - 6.9407 J/cm

@Temperature -50.0 - 0.000 °C
7.01 - 13.003 ft-lb/in

@Temperature -58.0 - 32.0 °F
Average value: 4.02 J/cm Grade Count:10
0.900 - 5.34 J/cm

@Temperature -40.0 - 0.000 °C
1.69 - 10.0 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 4.02 J/cm Grade Count:18
0.900 - 5.34 J/cm

@Thickness 3.17 - 3.20 mm
1.69 - 10.0 ft-lb/in

@Thickness 0.125 - 0.126 in
Average value: 4.02 J/cm Grade Count:18
Izod Impact, Unnotched 5340 J/cm - NB
10000 ft-lb/in - NB
Grade Count:3
Izod Impact, Notched (ISO) 9.00 - 94.0 kJ/m²
4.28 - 44.7 ft-lb/in²
Average value: 54.4 kJ/m² Grade Count:13
7.00 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 17.5 kJ/m² Grade Count:7
14.0 - 16.0 kJ/m²

@Temperature -30.0 - -30.0 °C
6.66 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 17.5 kJ/m² Grade Count:4
14.0 - 16.0 kJ/m²

@Thickness 3.20 - 3.20 mm
6.66 - 7.61 ft-lb/in²

@Thickness 0.126 - 0.126 in
Average value: 17.5 kJ/m² Grade Count:4
Izod Impact, Unnotched (ISO) NB
NB
Grade Count:5
NB - NB

@Temperature -30.0 - -30.0 °C
NB - NB

@Temperature -22.0 - -22.0 °F
Grade Count:5
Charpy Impact Unnotched 1000 J/cm² - NB
4760 ft-lb/in² - NB
Grade Count:17
999.9 J/cm² - NB

@Temperature -60.0 - -30.0 °C
4759 ft-lb/in² - NB

@Temperature -76.0 - -22.0 °F
Grade Count:10
Charpy Impact, Notched 3.00 - 7.00 J/cm²
14.3 - 33.3 ft-lb/in²
Average value: 5.50 J/cm² Grade Count:6
1.40 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
6.66 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.55 J/cm² Grade Count:4
1.40 - 1.60 J/cm²

@Thickness 3.00 - 3.00 mm
6.66 - 7.61 ft-lb/in²

@Thickness 0.118 - 0.118 in
Average value: 1.55 J/cm² Grade Count:4
Gardner Impact 36.0 - 36.2 J
26.6 - 26.7 ft-lb
Average value: 36.1 J Grade Count:7
Dart Drop, Total Energy 39.3 - 57.0 J
29.0 - 42.0 ft-lb
Average value: 49.1 J Grade Count:3
Falling Dart Impact 59.6561 - 59.6561 J

@Temperature -28.9 - -28.9 °C
44.0001 - 44.0001 ft-lb

@Temperature -20.0 - -20.0 °F
Average value: 59.7 J Grade Count:1
Puncture Energy 50.0 - 55.0 J
36.9 - 40.6 ft-lb
Average value: 51.5 J Grade Count:10
55.0 - 60.0 J

@Temperature -30.0 - -30.0 °C
40.6 - 44.3 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 56.5 J Grade Count:10
Thermal Properties Metric English Comments
CTE, linear 48.0 - 74.4 µm/m-°C
26.7 - 41.3 µin/in-°F
Average value: 65.6 µm/m-°C Grade Count:26
CTE, linear, Transverse to Flow 59.0 - 78.1 µm/m-°C
32.8 - 43.4 µin/in-°F
Average value: 67.6 µm/m-°C Grade Count:15
Specific Heat Capacity 1.70 - 1.77 J/g-°C
0.406 - 0.423 BTU/lb-°F
Average value: 1.72 J/g-°C Grade Count:8
Thermal Conductivity 0.173 - 0.214 W/m-K
1.20 - 1.49 BTU-in/hr-ft²-°F
Average value: 0.187 W/m-K Grade Count:12
Electrical Properties Metric English Comments
Electrical Resistivity 10.0 - 1.00e+17 ohm-cm
10.0 - 1.00e+17 ohm-cm
Average value: 1.60e+16 ohm-cm Grade Count:30
Surface Resistance 10000 - 1.00e+16 ohm
10000 - 1.00e+16 ohm
Average value: 2.17e+15 ohm Grade Count:26
Dielectric Constant 2.80 - 3.20
2.80 - 3.20
Average value: 3.05 Grade Count:14
Dielectric Strength 15.0 - 35.0 kV/mm
380 - 889 kV/in
Average value: 28.4 kV/mm Grade Count:20
Dissipation Factor 0.000400 - 0.0120
0.000400 - 0.0120
Average value: 0.00605 Grade Count:13
Arc Resistance 0.000 - 120 sec
0.000 - 120 sec
Average value: 86.7 sec Grade Count:6
Comparative Tracking Index 125 - 400 V
125 - 400 V
Average value: 213 V Grade Count:15
High Voltage Arc-Tracking Rate, HVTR 25.4 - 150 mm/min
1.00 - 5.91 in/min
Average value: 113 mm/min Grade Count:4