| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength |
17.7
kV/mm <br>@Thickness 3.20 mm
|
450
kV/in <br>@Thickness 0.126 in
|
in air; ASTM D149 |
|
SABIC Innovative Plastics Lexan® 500 PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance.
|
|||
| Dielectric Strength | 17.7 - 55.0 kV/mm | 450 - 1400 kV/in | Average value: 36.2 kV/mm Grade Count:20 |
|
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | ASTM D149 |
|
KKPC Kuhmo HI 450S High Gloss HIPS
Key features: High-gloss Common Uses: Portable CD-case, air conditioner cases.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impac..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | ASTM D149 |
|
KKPC Kuhmo HI 420T Transparent HIPS
Key features: Translucent Extrusion. Common Uses: Transparent toys, glass cases, various products made by injection molding needing contact-movability.HIPS is a functional resin made by copolymeriza..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | ASTM D149 |
|
KKPC Kuhmo HI 425TVD High Flow/High Heat Resistant HIPS
Key features: High-impact-fluidity. Common Uses: TV cover, computer case.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-res..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES Elastoblend® POM CO IM MB
Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact Modified and CopolymerInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® ABS GF30 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackTPCI# 1018121Information provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® HIPS GF15 15% Glass Filled
Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA11 GL8 HS UV
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Graphite Powder Lubricant and UV StabilizerFeatures: Heat Stabilized. Good UV Resistance and LubricatedAppearance: Natural ColorIn..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA12 CM40 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA6 GF50 L 50% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA6/6 GF/M40 L BK 40% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA6/6 GF35 HS L 35% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and heat StabilizedProcessin..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PES GF30 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES Luriblend® PA6 GF40 ML2 HS UV BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilized, Molybdenum Disulfide Lubricant and UV StabilizerFeatures: Lubricated, Good ..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES Luriblend® POM CO GF20 TL15 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionInf..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES Luriblend® POM CO X Acetal
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and CopolymerInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES Luriblend® POM HO TL2 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(2%)Features: Lubricated, Good Wear Resistance and HomopolymerInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill FR® PP FR-N X BKN001
Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Short Time; ASTM D149 |
|
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade
Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | 125 mil |
|
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin
Product Description: Master Bond Polymer System EP112M is a solventless, medium viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor ..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | |
|
Trelleborg Emerson & Cuming Stycast® 2760 Two-Component Easy Mix Ratio Encapsulant
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, ..
|
|||
| Dielectric Strength | >= 17.7 kV/mm | >= 450 kV/in | |
|
Dow Corning 7 RELEASE COMPOUND
Silicone-based compound, light consistencyInformation provided by Dow Corning
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | ASTM D149 |
|
Arlon LW401B##-P0 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
|
|||
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | |
|
Arkema Group Oroglas® SG 7 Acrylic, Gamma Radiation Resistant
(discontinued **)
OROGLAS SG 7 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no adverse ..
|
|||
| Dielectric Strength |
17.7
kV/mm <br>@Thickness 1.91 mm
|
450
kV/in <br>@Thickness 0.0750 in
|
|
|
Momentive Performance Materials RTV630 Blue General Purpose Potting/Encapsulating Compound
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..
|
|||
| Dielectric Strength |
17.7
kV/mm <br>@Thickness 3.20 mm
|
450
kV/in <br>@Thickness 0.126 in
|
in oil; ASTM D149 |
|
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Asia Pacific)
Glass reinforced. Flame retardant.
|
|||