Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 80.0 - 100 kV/mm | 2030 - 2540 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high.. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
PolyOne Bergamid™ A70 G25 H U-SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
PolyOne Bergamid™ A700 BK VN4255 LS Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
PolyOne Bergamid™ A700 blue VN4817CF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
PolyOne Bergamid™ A700 G20 U-SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PA320G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PA323G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60250 |
Polyram PlusTek PA340S4 Nylon 66 for Injection Molding, 20% Glass-Beads Reinforced 20% Glass-beads reinforced Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PA360G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced with molybdenum disulfide polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB300G5 Nylon 6, 15% Glass Fiber 15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60250 |
Polyram PlusTek PB302G50BK39P Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB304G7 Nylon 6, 35% Glass Fiber 35% glass-fiber reinforced, heat stabilized and impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB305G33 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized and UV stabilized polyamide 6 approved and listed by W.R.C and NSF/ANSI 61 international for potable waterInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB306G6 Nylon 6, 30% Glass Fiber 30% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60250 |
Polyram PlusTek RA325G6 Nylon 66 for Injection Molding, 30% Glass-Fiber Reinforced, Flame Retardant, Halogen Free 30% Glass-fiber reinforced, flame retardant halogen free Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek RA325J5 Nylon 6.6, 25% Glass beads and Glass Fiber, Flame Retardant 25% glass beads and glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 243; VDE 0303T2 |
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6) at 50% RH Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil.. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB303G6 Nylon 6, 30% Glass Fiber 30% Glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB321I6 Nylon 6, 30% Glass Fiber and Mineral 30% glass fiber and mineral reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60250 |
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized 50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60250 |
Polyram PlusTek PB826G3 Nylon 6 for Injection Molding, 15% Glass-fiber Reinforced, Impact Modified and UV Stabilized 15% Glass fiber reinforced, impact modified and UV stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | ASTM D149, IEC 243 |
EPICHEM Epinyl PA 6 GF 30 H Polyamide 6, 30% Glass, Heat Stabilized Characteristics: medium viscosity, 30% glass fibre, heat stabilized |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | ASTM D149, IEC 243 |
EPICHEM Epinyl PA 6 GF 30 Polyamide 6, 30% Glass Characteristics: medium viscosity, 30% glass fibre, excellent mechanical properties |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | ASTM D149, IEC 243 |
EPICHEM Epinyl PA 66 GF25 AU Polyamide 66, 25% Glass, Self extinguishing Characteristics: 25% glass fibre filled |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | ASTM D149, IEC 243 |
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Dielectric Strength | >= 80.0 kV/mm | >= 2030 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as.. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek RA320G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |