Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 80.0 - 100 kV/mm | 2030 - 2540 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high.. |
|||
Dielectric Strength | 70.0 - 100 kV/mm | 1780 - 2540 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIPA® (PA 6) Polyamide POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc.. |
|||
Dielectric Strength | 80.0 - 100 kV/mm | 2030 - 2540 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high.. |
|||
Dielectric Strength | 18.5 - 100 kV/mm | 470 - 2540 kV/in | Average value: 26.3 kV/mm Grade Count:49 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Dielectric Strength | 16.0 - 100 kV/mm | 406 - 2540 kV/in | Average value: 33.3 kV/mm Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Dielectric Strength | 70.0 - 100 kV/mm | 1780 - 2540 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIPA® (PA 6) Polyamide POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc.. |
|||
Dielectric Strength | 27.6 - 100 kV/mm | 701 - 2540 kV/in | Average value: 54.8 kV/mm Grade Count:49 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Dielectric Strength | 2.10 - 100 kV/mm | 53.3 - 2540 kV/in | Average value: 34.5 kV/mm Grade Count:8 |
Overview of materials for Polytetrafluoroethylene (PTFE) Powder This property data is a summary of similar materials in the MatWeb database for the category "PTFE Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Dielectric Strength | 17.0 - 100 kV/mm | 432 - 2540 kV/in | Average value: 33.0 kV/mm Grade Count:8 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Dielectric Strength | 11.8 - 100 kV/mm | 300 - 2540 kV/in | Average value: 29.3 kV/mm Grade Count:24 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Dielectric Strength | 1.00 - 100 kV/mm | 25.4 - 2540 kV/in | Average value: 33.0 kV/mm Grade Count:193 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Dielectric Strength | 60.0 - 100 kV/mm | 1520 - 2540 kV/in | DIN 53481 |
Isoflon TFM Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | 12.0 - 100 kV/mm | 305 - 2540 kV/in | Average value: 25.1 kV/mm Grade Count:53 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Dielectric Strength | 13.0 - 100 kV/mm | 330 - 2540 kV/in | Average value: 28.4 kV/mm Grade Count:20 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Dielectric Strength | 14.0 - 100 kV/mm | 356 - 2540 kV/in | Average value: 35.8 kV/mm Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Dielectric Strength | 17.0 - 100 kV/mm | 432 - 2540 kV/in | Average value: 24.9 kV/mm Grade Count:28 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Dielectric Strength | 11.8 - 100 kV/mm | 300 - 2540 kV/in | Average value: 26.8 kV/mm Grade Count:105 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Dielectric Strength | 15.0 - 100 kV/mm | 381 - 2540 kV/in | Average value: 27.8 kV/mm Grade Count:48 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Dielectric Strength | 19.7 - 100 kV/mm | 500 - 2540 kV/in | Average value: 56.3 kV/mm Grade Count:5 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Dielectric Strength | 15.0 - 100 kV/mm | 381 - 2540 kV/in | Average value: 28.1 kV/mm Grade Count:26 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |