Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 38.0 kV/mm | 965 kV/in | |
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical |
|||
Dielectric Strength | 38.0 kV/mm @Thickness 1.00 mm |
965 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Dielectric Strength | 38.0 kV/mm @Thickness 1.00 mm |
965 kV/in @Thickness 0.0394 in |
d.a.m.; IEC 60243-1 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | IEC 60243-1 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic.. |
|||
Dielectric Strength | 38.0 kV/mm @Thickness 1.00 mm |
965 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Ineos ABS Lustran® Ultra 4000 PG ABS Pellets (a-methylstyrene-SAN-modified), Electroplating Grade Lustran® Ultra 4000 PG is electroplating grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | K20/P20; IEC 60243-1 |
Styrolution Luran® S KR 2864 C Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | K20/P20; IEC 60243-1 |
Styrolution Luran® S KR 2864 C UV Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | IEC 60243-1 |
Styrolution Terblend® N NM-11 ABS/PA6 (Conditioned) Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | IEC 60243-1 |
Styrolution Terblend® N NMX04 ABS/PA6 (Conditioned) Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU.. |
|||
Dielectric Strength | 38.0 kV/mm @Thickness 1.50 mm |
965 kV/in @Thickness 0.0591 in |
Short Time; IEC 60243-1 |
Styrolution Novodur® H801 ABS / PC Novodur H801 is a high heat injection molding grade with high impact strength and reduced emission.Information provided by Styrolution |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | ASTM D149 |
Westlake Plastics Zelux® M Machine Grade Polycarbonate Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | |
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber Only opaque colors available, with 20% glass fiber reinforcement, flame retardant.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | cond; IEC 60243-1 |
DSM EcoPaXX® Q-X07208 PA410-I-GF30 % Glass Reinforced, Impact Modified |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
DSM EcoPaXX® Q-X07209 PA410-I-GF40 % Glass Reinforced, Impact Modified |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® AG-30 PA66-GF30 Information provided by EMS Grivory |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® AG-35 PA66-GF35 Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers. High stiffnessHigh tensile strengthHigh heat distortion temperatureEasy .. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30 Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: .. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50 Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4063 black 9238 PA6T/66-GF30 Product description: Grivory XE 4063 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4188 black 9992 PA612 Product description: Grilamid XE 4188 black 9992 is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 black 9992 are: High v.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | |
Arkema Group Orgalloy® RS 6000 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Dielectric Strength | 38.0 kV/mm @Thickness 1.00 mm |
965 kV/in @Thickness 0.0394 in |
ASTM D149 |
Arkema Group Orgalloy® RS 6000 Polyamide 6 Alloy Polyamide Alloy, Rigid grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | K20/P20; IEC 60243-1 |
Styrolution Luran® S KR 2863 C UV Colored ASA+PC Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | |
Arkema Group Orgalloy® R 60ES Nylon 6 Alloy (Conditioned) Rigid polyamide 6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents). Blow extrusion grade for technical films: thermal resistance, barrier to gases and aromas,.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | |
Arkema Group Orgalloy® RS 60E10 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |