Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 150 sec | 150 sec | |
Pyrotek TS-120 Thermoset Electrical Insulation Product (Nema Grade: GPO-2) Glass reinforcement, Polyester resin, Cream color. Highly flame resistant. Meets UL 94VO.Information provided by Pyrotek. |
|||
Arc Resistance | 150 sec | 150 sec | Average value: 150 sec Grade Count:6 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Arc Resistance | 150 - 180 sec | 150 - 180 sec | Average value: 165 sec Grade Count:6 |
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and .. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Plenco 4246 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 04246 flow 18 is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, moldability and molded finish characteristics. It is use.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Plenco Valite 4100 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
(discontinued **) Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Highest physical properties of GLASROD series. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Haysite ETS Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A NEMA GPO-1 economy grade fiberglass mat reinforced thermoset polyester molded sheet. ETS is an IEEE Class B 130ºC electrical/160ºC mechanical material with good punching characteristics. Typ.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Haysite H258 Polyester Laminate Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Haysite H722 Polyester, Glass Reinforced H722 is an all-purpose GPO-1 fiberglass mat reinforced thermoset polyester molded sheet. Available in thicknesses ranging from .031" - 2.00". Standard color - Natural. Meets Gov't Specs - LP-509, .. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Haysite H755 Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A new generation of IEEE Class F, 155ºC /165ºC NEMA GPO- 1 material. H755 is designed to bridge the gap between 130ºC Class B GPO-1 materials and Class H 180ºC grades. H755 has quickly g.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Haysite HCR-196 Corrosion Resistant Vinyl Ester/Glass Sheet A fiber glass reinforced thermoset sheet using DEREKANE® 470 vinylester in the resin matrix. Standard color is grey. Additional data covering resistance to specific chemicals is available upon re.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Glastic Laminates/Shapes UTR Pultruded Tubing, Fiberglass-Reinforced Polyester Data provided by Glastic Corporation.NEMA GPO-3, NEMA LI-1. Commonly used for tubing and fuse applications. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D-495 |
Glastic SG-200 Corner Angles Corner angles used for coil winding.Information provided by Glastic Corporation |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Samyang Tribit® 1500G10 PBT, Reinforced General Purpose Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G10 is a reinforced, general purpose gr.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 2-501N Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 2-520 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Arc Resistance | >= 150 sec | >= 150 sec | Dry; ASTM D495 |
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e.. |
|||
Arc Resistance | >= 150 sec | >= 150 sec | |
Abatron AboCast 8103-21 High-Performance Dielectric Epoxy AboCast 8103-21 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system combines r.. |
|||
Arc Resistance | >= 150 sec | >= 150 sec | |
Abatron AboCast 8103-24 High-Performance Dielectric Epoxy AboCast 8103-24 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has an exc.. |
|||
Arc Resistance | >= 150 sec | >= 150 sec | |
Abatron AboCast 8103-20 High-Performance Dielectric Epoxy AboCast 8103-20 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is unique .. |
|||
Arc Resistance | >= 150 sec | >= 150 sec | |
Abatron AboCast 8103-23 High-Performance Dielectric Epoxy AboCast 8103-23 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has a comb.. |
|||
Arc Resistance | >= 150 sec | >= 150 sec | |
Abatron AboCast 8103-25 High-Performance Dielectric Epoxy AboCast 8103-25 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system combines o.. |
|||
Arc Resistance | >= 150 sec | >= 150 sec | |
Abatron AboCast 8103-22 High-Performance Dielectric Epoxy AboCast 8103-22 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is used in.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Chevron Phillips Ryton® R-7 02 Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® R-7 02 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compound wit.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Plenco 4311 Phenolic, Granular, Transfer Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Arc Resistance | 150 sec | 150 sec | ASTM D495 |
Chang Chun Plastic Longlite PM T375J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Arc Resistance | 150 sec | 150 sec | |
Cosmic Plastics 3D36 Thermoset Polyester Molding Compound Data provided by the manufacturer. |