| Category | Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS |
| Manufacturer | Glastic |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Glastic SG-200 Corner Angles.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.85 g/cc | 1.85 g/cc | ASTM D-792 |
| Water Absorption | 0.15 % | 0.15 % | % by wt.; ASTM D-570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 483 MPa | 70000 psi | ASTM D-638 |
| Tensile Modulus | 20.7 GPa | 3000 ksi | ASTM D-638 |
| Flexural Strength | 552 MPa | 80000 psi | ASTM D-790 |
| Flexural Modulus | 26.9 GPa | 3900 ksi | ASTM D-790 |
| Compressive Strength | 96.5 MPa | 14000 psi | Transverse; ASTM D-695 |
| 345 MPa | 50000 psi | Axial; ASTM D-695 | |
| Shear Strength | 20.7 MPa | 3000 psi | In plane; ASTM D-3914 |
| Izod Impact, Notched | 21.4 J/cm | 40.0 ft-lb/in | ASTM D-256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
| Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C-177 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Insulation Resistance | 6.40e+15 ohm | 6.40e+15 ohm | ASTM D-257 |
| Dielectric Constant | 5.0 @Frequency 60 Hz |
5.0 @Frequency 60 Hz |
ASTM D-150 |
| Dielectric Strength | 2.80 kV/mm | 71.1 kV/in | 1" Axial in Oil; ASTM D-149 |
| Arc Resistance | 150 sec | 150 sec | ASTM D-495 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Standard Color | Tan |