Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 8103-21 High-Performance Dielectric Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8103-21 High-Performance Dielectric Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AboCast 8103-21 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system combines rigidity, heat resistance, and good thermocycling properties.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Part B
1.14 g/cc
0.0411 lb/in³
Part A
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.2 MPa
8000 psi
Elongation at Break 27 %
27 %
Tensile Modulus 5.45 GPa
790 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Deflection Temp at unknown load
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
Dielectric Constant 2.9

@Frequency 60.0 Hz,
Temperature 23.0 °C
2.9

@Frequency 60.0 Hz,
Temperature 73.4 °F
3.2

@Frequency 60.0 Hz,
Temperature 100 °C
3.2

@Frequency 60.0 Hz,
Temperature 212 °F
3.3

@Frequency 60.0 Hz,
Temperature 150 °C
3.3

@Frequency 60.0 Hz,
Temperature 302 °F
Dissipation Factor 0.010

@Frequency 60.0 Hz,
Temperature 23.0 °C
0.010

@Frequency 60.0 Hz,
Temperature 73.4 °F
0.031

@Frequency 60.0 Hz,
Temperature 100 °C
0.031

@Frequency 60.0 Hz,
Temperature 212 °F
0.080

@Frequency 60.0 Hz,
Temperature 150 °C
0.080

@Frequency 60.0 Hz,
Temperature 302 °F
Arc Resistance >= 150 sec
>= 150 sec
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 100 °C
2.00 - 3.00 hour

@Temperature 212 °F
60.0 - 240 min

@Temperature 120 - 160 °C
1.00 - 4.00 hour

@Temperature 248 - 320 °F
optional
Pot Life 30 min

@Temperature 80.0 °C
30 min

@Temperature 176 °F
>= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Descriptive Properties Value Comments
Arc-Track Free (min) > 2000
2.5 KV
Color Clear
Parts by Weight (pbw) 100
Part A
65
Part B
Thermal Shock Resistance Scale 0 (poor) to 10 (excellent)