Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 8103-24 High-Performance Dielectric Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Abatron AboCast 8103-24 High-Performance Dielectric Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AboCast 8103-24 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has an exceptional combination of rigidity, heat and thermocycling resistance.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0411 lb/in³
Part A
1.17 g/cc
0.0424 lb/in³
Part B
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.1 MPa
6100 psi
Elongation at Break 11 %
11 %
Tensile Modulus 1.54 GPa
223 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 163 °C
325 °F
Deflection Temp at unknown load
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Constant 3.3
<br>@Frequency 60.0 Hz,<br> Temperature 23.0 °C
3.3
<br>@Frequency 60.0 Hz,<br> Temperature 73.4 °F
3.79
<br>@Frequency 60.0 Hz,<br> Temperature 100 °C
3.79
<br>@Frequency 60.0 Hz,<br> Temperature 212 °F
4.6
<br>@Frequency 60.0 Hz,<br> Temperature 150 °C
4.6
<br>@Frequency 60.0 Hz,<br> Temperature 302 °F
Dissipation Factor 0.0090
<br>@Frequency 60.0 Hz,<br> Temperature 23.0 °C
0.0090
<br>@Frequency 60.0 Hz,<br> Temperature 73.4 °F
0.027
<br>@Frequency 60.0 Hz,<br> Temperature 100 °C
0.027
<br>@Frequency 60.0 Hz,<br> Temperature 212 °F
0.073
<br>@Frequency 60.0 Hz,<br> Temperature 150 °C
0.073
<br>@Frequency 60.0 Hz,<br> Temperature 302 °F
Arc Resistance >= 150 sec
>= 150 sec
Processing Properties Metric English Comments
Cure Time 120 - 180 min
<br>@Temperature 100 °C
2.00 - 3.00 hour
<br>@Temperature 212 °F
60.0 - 240 min
<br>@Temperature 120 - 160 °C
1.00 - 4.00 hour
<br>@Temperature 248 - 320 °F
optional
Pot Life 30 min
<br>@Temperature 80.0 °C
30 min
<br>@Temperature 176 °F
>= 480 min
<br>@Temperature 25.0 °C
>= 480 min
<br>@Temperature 77.0 °F
Descriptive Properties Value Comments
Arc-Track Free (min) > 2000
2.5 KV
Color Opaque
Parts by Weight (pbw) 100
Part A
75
Part B
Thermal Shock Resistance Scale 0 (poor) to 10 (excellent)
Copyright © lookpolymers.com All Rights Reserved